Ring-shaped specimens cored from light grey granite were tested in tension using two distinct approaches: a direct configuration based on a modified seesaw test (MST) and an indirect configuration based on diametral compression of rings. In the MST method, tensile loading was applied at the inner diameter by means of a lever-driven fixture. A lever-arm correction was incorporated to convert actuator load to the effective load transmitted to the specimen, and geometric effects were accounted for through a dimensionless shape factor. In contrast, the IR method estimated tensile strength from external diametral compression using an indirect formulation and its own geometry-dependent factor. The MST results produced an average tensile strength of approximately 7.32 MPa with a standard deviation of 0.29 MPa. The IR method produced a higher average tensile strength of approximately 8.78 MPa with a standard deviation of 0.27 MPa for rings of comparable geometry. The difference between the two methods indicates that the indirect ring approach tends to report a higher apparent tensile resistance than the MST. This increase is attributed to indirect loading, stress redistribution, and contactinduced confinement, rather than to a true increase in cohesive tensile capacity of the granite. The results demonstrate that (i) direct inner-diameter loading of ring specimens can be implemented through a calibrated lever system, (ii) the required lever correction and geometry factor can be expressed in closed form, and (iii) the modified seesaw method can be used to obtain reproducible tensile strength values that are mechanically traceable to force equilibrium.
The shift toward low-carbon and climate-resilient infrastructure has accelerated the development of advanced cementitious materials and reinforcement systems. This review summarizes recent progress in supplementary cementitious materials (SCMs), limestone–calcined clay cement (LC3), alkali-activated binders, CO2-cured concretes, and recycled-aggregate concretes, focusing on their contributions to clinker reduction, durability enhancement, and circular resource use. Performance is analysed across major exposure conditions, including chloride ingress, sulphate environments, carbonation, and freeze–thaw cycles. Waste-derived additives such as glass powder, crumb rubber, and recycled plastics are assessed for their functional benefits and engineering limitations. The paper also reviews self-healing technologies—capsule-based, crystalline, and microbial—that improve crack sealing, reduce permeability, and delay corrosion. Additionally, the role of FRP reinforcement in providing corrosion-free alternatives for aggressive environments is examined.
This chapter develops a comprehensive unified inverse analytical framework for the simultaneous determination of tensile strength and elastic modulus from indirect tensile tests on brittle geomaterials, with specific application to underground energy infrastructure in smart cities. The framework systematically integrates finite contact mechanics, annular specimen geometry, and combined machine–specimen compliance interactions into a coherent semi-analytical forward model. An inverse identification procedure, formulated as a weighted nonlinear least-squares problem and solved via the Levenberg–Marquardt algorithm with analytically derived Jacobians, extracts both material parameters directly from the complete load–displacement curve, bypassing the traditional reliance on peak load alone. Uncertainty quantification is incorporated through covariance analysis of the identified parameter estimates. The methodology is applicable to Brazilian disc, annular Brazilian, and modified seesaw test configurations and is validated through energy-based consistency arguments.
This study presents a comprehensive analytical-numerical framework for characterizing the progressive contact phenomena in Brazilian ring discs. By solving a dual trigonometric series representation of the contact problem, the model enables precise determination of contact pressure distributions, angular extents, and the ensuing load–displacement relationships. The proposed analytical methodology is rigorously validated against finite element method (FEM) simulations. Under diametral compression conditions, the numerical approach yields a peak load (P) and displacement (δ) of 25.2 kN and 0.0362 mm, respectively, which exhibit minor deviations (approximately 7.93% under a 10% load variation) relative to FEM-predicted values (23.2 kN and 0.0340 mm).The analysis reveals a progressive expansion of the contact half-angle under diametral compression, initially involving a small stress-intensive segment and incrementally increasing to approximately 7° at 25% load, 13° at 50% load, and nearly 20° immediately before fracture initiation. Finite element simulations closely replicated this contact-angle evolution, achieving about 20° at peak load.