Triangular Heisenberg antiferromagnets are prototypes of geometric frustration, even if for nearest-neighbor interactions quantum fluctuations are not usually strong enough to destroy magnetic ordering: stronger frustration is required to stabilize a spin-liquid phase. On the basis of static magnetization and electron spin resonance measurements, we demonstrate the emergence of moments in the triangular-lattice magnet . These moments are subject to an extra source of frustration that causes magnetic correlations to set in far above both the magnetic ordering and Weiss temperatures. Corroborating the ground state, theory identifies ferromagnetic Kitaev exchange anisotropy as an additional frustrating agent, altogether putting forward as a promising Kitaev spin-liquid material.
A judicious analysis of previously published experimental data leads one to conclude that the ground state of iron(II) phthalocyanine is an orbitally degenerate spin triplet \documentclass[12pt]{minimal}\begin{document}$a_{1g}^2 e_g^{\uparrow \downarrow \uparrow } b_{2g}^{\uparrow }$\end{document}a1g2eg↑↓↑b2g↑ (3Eg). The ligand field parameters, in relation to Racah's C, are approximately as follows: B20/C = 0.84, B40/C = 0.0074. The uniqueness of this result is demonstrated by means of a special diagram in the B20/C − B40/C plane (under additional conditions that B44/B40 = 35/3 and B/C = 0.227). The system is in a strong-ligand-field regime, which enables the use of single-determinant techniques corrected for correlations within the 3d shell of Fe.
Pure and cobalt-doped zinc oxide aligned nanorods have been grown by the low-temperature (90 °C) aqueous chemical method on amorphous ZnO seed layer, deposited on a sapphire substrate. High crystallinity of these objects is demonstrated by the electron paramagnetic resonance investigation at liquid helium temperature. The successful incorporation of Co 2+ ions in substitution of Zn 2+ ones in the ZnO matrix has also been confirmed. A drastic reduction of intrinsic ZnO nanorods core defects is observed in the Co-doped samples, which enhances the structural quality of the NRs. The quantification of substitutional Co 2+ ions in the ZnO matrix is achieved by comparison with a reference sample. The findings in this study indicate the potential of using the low-temperature aqueous chemical approach for synthesizing material for spintronics applications.
Zinc oxide (ZnO) nanorods grown by the low-temperature (90 °C) aqueous chemical method with different cobalt concentration within the synthesis solution (from 0% to 15%), are studied by electron paramagnetic resonance (EPR), just above the liquid helium temperature. The anisotropic spectra of substitutional Co 2+ reveal a high crystalline quality and orientation of the NRs, as well as the probable presence of a secondary disordered phase of ZnO:Co. The analysis of the EPR spectra indicates that the disappearance of the paramagnetic native core-defect (CD) at is correlated with the apparition of the Co 2+ ions lines, suggesting a gradual neutralization of the former by the latter. We show that only a little amount of cobalt in the synthesis solution (about 0.2%) is necessary to suppress almost all these paramagnetic CDs. This gives insight in the experimentally observed improvement of the crystal quality of diluted ZnO:Co nanorods, as well as into the control of paramagnetic defects in ZnO nanostructures.
We demonstrate an efficient possibility to synthesize vertically aligned pure zinc oxide (ZnO) and Co-doped ZnO nanorods (NRs) using the low-temperature aqueous chemical synthesis (90 °C). Two different mixing methods of the synthesis solutions were investigated for the Co-doped samples. The synthesized samples were compared to pure ZnO NRs regarding the Co incorporation and crystal quality. Electron paramagnetic resonance (EPR) measurements confirmed the substitution of Co2+ inside the ZnO NRs, giving a highly anisotropic magnetic Co2+ signal. The substitution of Zn2+ by Co2+ was observed to be combined with a drastic reduction in the core-defect (CD) signal (g ∼ 1.956) which is seen in pure ZnO NRs. As revealed by the cathodoluminescence (CL), the incorporation of Co causes a slight red-shift of the UV peak position combined with an enhancement in the intensity of the defect-related yellow-orange emission compared to pure ZnO NRs. Furthermore, the EPR and the CL measurements allow a possible model of the defect configuration in the samples. It is proposed that the as-synthesized pure ZnO NRs likely contain Zn interstitial (Zni+) as CDs and oxygen vacancy (VO) or oxygen interstitial (Oi) as surface defects. As a result, Co was found to likely occupy the Zni+, leading to the observed CDs reduction and hence enhancing the crystal quality. These results open the possibility of synthesis of highly crystalline quality ZnO NRs-based diluted magnetic semiconductors using the low-temperature aqueous chemical method.