In the present research, chitosan/collagen and chitosan/collagen/nano-hydroxyapatite (nHAP) hydrogel nanocomposites were prepared using naturally extracted chitosan from Persian Gulf shrimp wastes and rat tail-tendon collagen. Freeze-gelation method was used to prepare highly porous scaffolds. The morphology, chemical structure, water retainability, and thermal properties were characterized using SEM, FTIR, water content experiment, simultaneous thermal analysis (STA), respectively. Atomic force microscopy (AFM) nanoindentation and unconfined compression test were used to assess different feature of the mechanical properties of the hydrogels. The obtained results were so promising that the prepared nanocomposites can be considered as a potential candidate for cartilage tissue engineering.
This study outlines the optimization of photocatalytic degradation of toluene by W-doped TiO2 nanoparticles under visible light irradiation. Experiments were carried out based on the central composite design (CCD) methodology. W-TiO2 nanoparticles were synthesized with various tungsten contents at different calcination temperatures by the sol–gel method. The nanoparticles’ characteristics were determined using appropriate techniques such as field emission scanning electron microscopy, particle size analysis, X-ray diffraction and energy-dispersive spectroscopy. The effect of different operational conditions of coating mass, initial toluene concentration, and exposure time on the toluene removal efficiency was investigated. Result showed that tungsten has a fundamental role in improving the photocatalytic activity of TiO2 under visible light, as well as improving its photoactivity under UV irradiation by decreasing the rate of electron/hole charge recombination. Analysis of the obtained data on toluene removal with a CCD approach illustrated that the quadratic model can effectively predict the toluene removal with coefficient of determination of R2 = 0.862. Tungsten content and exposure time affect the toluene removal efficiency more than other factors. Results showed that maximum toluene removal efficiency slightly depends on the initial concentration of toluene. At the initial toluene concentration of 4000 ppm, the optimum values of the calcination temperature, tungsten content, coating mass, and exposure time were 500°C, 0.52 wt%, 11.7 g/m2, and 8 h, respectively, with 59% removal of toluene.
24 July 2017 in International Journal of Polymeric Materials and Polymeric Biomaterials
The mechanical property is a crucial factor in the design of bone tissue engineering scaffolds. In the current study, novel PLLA (Poly-L-lactic acid)–Hydroxyapatite (HA)–yttria-stabilized zirconia (YSZ) nanocomposite scaffold with various compositions was prepared and characterized. The effect of HA and YSZ contents on the mechanical behavior of the resultant composites was investigated. TEM micrograph revealed that HA particles are needle-like in shape and nano in size. Scanning electron microscopy (SEM) micrograph also showed that YSZ powder is in granule form and submicron size. SEM disclosed that all scaffolds had a highly interconnected porous structure and X-ray diffractometry revealed that there were some molecular interactions between PLA (Polylactic acid), HA, and YSZ in the composites. The results depicted that introducing YSZ to the nanocomposite leads to a significant increase in compressive strength, modulus, and densification strain. In addition, flexural strength and modulus showed an upward trend by adding YSZ particles to scaffolds. It should be noted that PLA–20%HA–20%YSZ indicates the highest strength and modulus in both compression and bending tests, though, it did not demonstrate the proper strain compared to other scaffolds. Thus, PLA–15%HA–15%YSZ has been reported as the best candidate due to appropriate strength and strain. Also, energy absorption in nanocomposites showed an upward trend by increasing the amount of YSZ particles. It was found that the strength of samples was declined after being soaked in simulated body fluid. However, scaffolds with HA underwent more decrease in strength compared to samples containing YSZ.