19 May 2009 in IEEE Transactions on Magnetics
Verified
Journal Article
Closed access
KTKontan Tarigan
Kontan Tarigan
YYYong-Goo Yoo
Yong-Goo Yoo
DYDong-Seok Yang
Dong-Seok Yang
JGJean-Marc Greneche
Jean-Marc Greneche
SYSeong-Cho Yu
Seong-Cho Yu
Fe55Mn10Al35 alloys were prepared by mechanical alloying. Local ordering around the central atom was examined with milling time by using extended X-ray absorption fine structure. The structural and magnetic evolution was analyzed by EXAFS and Mossbauer study as a function of milling time. The first shell of the Fourier transformed spectra changed with milling time, indicating a change in the local ordering around the central Fe atom. X-ray diffraction patterns indicate a bcc phase after 24 h milling time. For 1 h milled sample, Mossbauer spectra analysed three sextets as bcc-Fe phase, broad sextet and Fe surrounded Al and Mn phase. The magnetization showed decrease with milling time corresponding to magnetic dilution.

9 July 2025 in Materials
Verified
Journal Article
Open access
PDF file
Dianta Ginting, EMBADianta Ginting, EMBA
Dianta Ginting, EMBA
HPHadi Pranoto
Hadi Pranoto
NUNurato
Nurato
KTKontan Tarigan
Kontan Tarigan
SASagir Alva
Sagir Alva
Jong-Soo RhyeeJong-Soo Rhyee
Jong-Soo Rhyee
The shortage of tellurium and toxicity of lead are major obstacles to scaling mid-temperature thermoelectric generators. We engineer quaternary lead chalcogenides with composition (Pb0.8Ge0.2Te)0.95-x(PbSe)0.05(PbS)x (0 ≤ x ≤ 0.25), where Pb is lead, Ge is germanium, Te is tellurium, Se is selenium, S is sulfur, and x denotes the molar fraction of lead sulfide (PbS). The primary novelty lies in achieving ultra-low thermal conductivity through controlled phase segregation induced by systematic PbS incorporation. X-ray diffraction analysis reveals single-phase solid solutions up to x ≈ 0.10, with secondary PbS precipitates forming beyond this threshold. These PbS-rich phases create hierarchical microstructures that scatter phonons across multiple length scales, suppressing total thermal conductivity to 0.6 Wm−1K−1 at x = 0.15—approximately 84% lower than pristine lead telluride (PbTe) and approaching glass-like thermal conductivity values. Electrical transport measurements demonstrate sulfur’s role as an electron donor, enabling carrier-type control from p-type to n-type conduction. Despite moderate electrical power factors, the optimized composition (x = 0.20) achieves a peak dimensionless figure of merit ZT ≈ 0.34 at 650 K. This work demonstrates an effective strategy for tellurium-lean, lead-reduced thermoelectric materials through sulfur-induced phase segregation, providing practical design guidelines for sustainable waste heat recovery applications.

1 March 2018 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
KTKontan Tarigan
Kontan Tarigan
DSD. Sebayang
D. Sebayang
SYS. C. Yu
S. C. Yu
DYD. S. Yang
D. S. Yang
The structural and the magnetic properties of nanocrystalline Fe 50 Cr 40 Si 10 alloys were prepared via mechanical alloying by using Fe, Cr, and Si elements with 1- to 24 hrs milling times. Structural analysis based on X-ray diffraction and Extended X-ray absorption fine structure spectroscopy. Concerning the magnetic behavior, the data obtained from a vibrating sample magnetometer at 300 K shows that both the magnetic saturation and the coercivity are dependent strongly on the milling time and the crystallite size. By adjusting the milling time, both appropriate structural transformation and magnetization values are obtained.

31 October 2025 in JTTM : Jurnal Terapan Teknik Mesin
Verified
Journal Article
Open access
PDF file
AUArie Umarwan
Arie Umarwan
KTKontan Tarigan
Kontan Tarigan
Silicone elastomers are widely used in industrial applications due to their mechanical properties and resistance to temperature and chemicals. In the manufacturing sector, particularly in bottle and jar capping machines, silicone is utilized as the base material for rollers operating under high dynamic loads. These conditions often lead to rapid wear and degradation of the silicone rollers during production processes. This study aims to review various literature sources related to the optimal composition and reinforcement methods for silicone elastomers to determine suitable formulations for roller capping applications. The research was conducted through a literature review of scientific journals published within the last ten years, focusing on the influence of filler type, crosslinker type, and composition on mechanical properties such as tensile strength, tear strength, and elongation at break. The review results indicate that a combination of fumed silica (0.2 phr) and clay (1 phr), along with a peroxide-based crosslinker (3 phr), provides the best mechanical performance, achieving a tensile strength of 6.9 MPa, tear strength of 21.5 kN/m, and elongation at break of 315%. In conclusion, the optimal reinforcement of silicone elastomers depends on the type of filler and crosslinking system used, which directly affects the material’s strength, elasticity, and thermal resistance

30 October 2017 in Journal of Physics: Conference Series
Verified
Conference Paper
Open access
PDF file
KTKontan Tarigan
Kontan Tarigan
YKY. Kusuma
Y. Kusuma
DSD. Sebayang
D. Sebayang
DYD. S. Yang
D. S. Yang
The structural and the magnetic properties of nanocrystalline Fe47.5Mn47.5C5 alloys were prepared by using a mechanical alloying technique, used the commercial Fe, Mn, and C powders as precursors. It was studied in detail as function of the milling times of 1- to 48 hrs. The structural analysis based on X-ray diffraction and extended X-ray absorption fine structure spectroscopy revealed that the alloying process took place after 36 hrs milling. Concerning the magnetic behavior, the data obtained from a vibrating sample magnetometer showed that both the magnetic saturation and the coercivity depended strongly on the milling time and the crystallite size. With these results, by adjusting the milling time shows that an appropriate structural transformation and appropriate magnetization value.

5 August 2016 in International Journal of Innovation in Mechanical Engineering and Advanced Materials
Verified
Journal Article
Open access
PDF file
KTKontan Tarigan
Kontan Tarigan
DSD. Sebayang
D. Sebayang
In this work, the formations of Fe55Mn10Al35 nanocrystalline alloys were made by using mechanical alloying (MA) technique with the milling time of 24 hrs and then annealed at 300, 500, and 700oC. The sizes and the morphology of the particles were checked by using a Scanning Electron Microscope (SEM). The magnetic properties were characterized by using a Vibration Sample Magnetometer (VSM), and it give results both of the magnetic saturation (Ms) and Coercivity (Hc) are decreased respect to annealing temperatures. Last one; the structures were characterized by using an Extended X-ray Absorption Fine Structure (EXAFS) and X-Ray Diffraction (XRD). It give results that the structures were single phase at 24 hrs milled and 300oC annealed, then the structure to be changed at 500 and 700oC.