A thermal-oxidative aging test at 120 °C was conducted on ethylene propylene diene monomer (EPDM) vulcanizates of the semi-efficient vulcanization system. The effect of thermal-oxidative aging on EPDM vulcanizates was systematically studied by curing kinetics, aging coefficient, crosslinking density, macroscopic physical properties, contact angle, Fourier Transform Infrared Spectrometer (FTIR), Thermogravimetric analysis (TGA) and thermal decomposition kinetics. The results show that the content of hydroxyl and carbonyl groups as well as the carbonyl index increased with increasing aging time, indicating that EPDM vulcanizates were gradually oxidized and degraded. As a result, the EPDM vulcanized rubber chains were crosslinked with limited conformational transformation and weakened flexibility. The thermogravimetric analysis demonstrates that the thermal degradation of EPDM vulcanizates had competitive reactions of crosslinking and degradation, and the thermal decomposition curve can be divided into three stages; meanwhile, the thermal stability of EPDM vulcanizates gradually decreased with increasing aging time. The introduction of antioxidants in the system can promote the crosslinking speed and reduce the crosslinking density of EPDM vulcanizates while inhibiting the surface thermal and oxygen aging reaction. This was attributed to the fact that the antioxidant can reduce the thermal degradation reaction level, but it is not conducive to the formation of a perfect crosslinking network structure and reduces the activation energy of thermal degradation of the main chain.
Maleic anhydride (MAH)–divinyl benzene (DVB) multi-monomer melt-grafting onto isotactic polybutene-1 (iPB-1) was carried out in a torque rheometer. The effects of dicumyl peroxide (DCP), MAH, and DVB concentrations, and temperature, on the reaction, were investigated. The optimized conditions were 170 °C, DVB/MAH = 4:6 (mass ratio). DVB as a comonomer enhanced the grafting degree (Gd) and grafting efficiency (Ge) of iPB-g-MAH better than styrene. The initiator DCP had little effect on Gd as its concentration over 0.2 phr, but the grafts’ melt flow rate (MFR) increased significantly, and relative molecular weight decreased remarkably with increased DCP concentration. With increasing Gd, the contact angle of grafts with water decreased, and there was a larger crystallization rate. The study of iPB-1 and iPB-g-MAH (Gd = 1.5%)-modified polyamide 6 (PA6) showed that iPB-g-MAH had an obviously toughening effect on PA6. With increasing iPB-g-MAH concentration, the blends of impact strength and elongation at break increased obviously, tensile strength decreased slightly, and MFR decreased prominently, which greatly slowed the processing degradation of PA6. The properties of iPB-1/PA6 blends deteriorated. Both DSC curves and SEM micrographs confirmed that PA6/iPB-g-MAH blends had much better compatibility than PA6/iPB. The reason was that the anhydride group in iPB-g-MAH reacted with amide group in PA6 to improve the compatibility between two phases, and iPB-g-MAH is an excellent modifier for PA6.
Maleic anhydride (MAH) grafting onto isotactic polybutene-1 (iPB-1) was prepared using di-tert-butyl peroxide (DTBP) as the initiator in the internal mixer. The influence of the reaction temperature, rotor rate, initiator content, monomer and co-monomer content, on grafting ratio (G/%) and melt flow rate (MFR), was investigated. The results showed that the temperature and rotor rate had little effect on the grafting ratio and MFR when the temperature was 160°C–200°C, and the rotor rate was 50 rpm–90 rpm. Besides, as the initiator content increased, the grafting ratio increased, but excessive initiator content led to degradation of macromolecules and a significant increase in MFR. The grafting ratio reached a peak value with an MAH content of 4.5 phr and a fixed initiator content of 0.3 phr. As a co-monomer, styrene (St) can enhance the G/% and decrease the MFR. The crystallization properties of iPB-1 were also studied. The grafting of MAH onto iPB-1 remarkably accelerated the crystal form II to I transformation of iPB-1 and the transformation rate increased with an increase in the G/% of iPB-1.