Polyurethane elastomers coating were synthesised by using typical diisocyanates, polyether and polyester polyols and HO-tertiary amines or diols as a chain extenders. Mole fractions of structural fragments (κexp) responsible for the polar interactions within polyurethane chains were calculated by 1H NMR method. Obtained results were confronted with the analogous parameter values (κtheor) calculated on the basis of process stoichiometry, considering the stage of the production of isocyanate prepolymers and reaction of their extension for polyurethanes. Trials of linear correlation between the κexp parameters and surface free energy (SFE) values of investigated coatings were presented. SFE values were determined by Owens–Wendt method, using contact angles measured with the goniometric method. Based on achieved results, another empirical models, allowing for prediction the influence of the kind of polyurethane raw materials on SFE values of received coatings were determined. It was found that it is possible to regulate the SFE in the range millijoules per cubic metre by the selection of appropriate substrates. It has been found that use of 2,2,3,3-tetrafluoro-1,4-butanediol as a fluorinated extender of prepolymer chains is essential to obtain coatings with increased hydrophobicity, applied among others as biomaterials—next to diphenylmethane diisocyanate and polyoxyethylene glycol.
The curing behaviour of the composition of a liquid-crystalline diepoxy monomer (LCEM) with the central triaromatic mesogenic group was studied using differential scanning calorimetry, conventional DSC and temperature-modulated TMDSC and nuclear magnetic resonance 1H-NMR spectroscopy. The stoichiometric amount of primary aromatic diamine, 4,4′-diaminodiphenylmethane (DDM), was used as a curing agent. TMDSC TOPEM® allowed the separation of the thermal effects related to reversible processes (e.g. phase transitions) from irreversible processes (cross-linking reaction) and determining that irreversible curing reaction occurs at the same time as reversible transition of the LCEM from crystal to the liquid-crystalline nematic phase. Additionally, 1H-NMR analysis of the LCEM/DDM mixture preheated to a temperature from the temperature range of complex thermal changes was conducted. The obtained spectrum clearly showed the presence of partially cured products in the investigated samples and additionally proved that during the endothermic phase transition of the LCEM monomer an exothermic cross-linking reaction was occurring.