Additive manufacturing is becoming more and more significant for the production of engineering products. The global community of designers and manufacturers will undoubtedly benefit from identifying the process factors that could lead to superior mechanical behaviour. The incorporation of fibres and nanoparticles in polymer matrix is one of the most significant advancements in polymer fabrication. This study intends to investigate how the flexural behaviour of dissimilar polymer composites viz carbon fibre reinforced poly lactic acid (CF-PLA), carbon fibre reinforced poly ethylene terephthalate glycol (CF-PETG) and multi walled carbon nano tubes reinforced PLA (MWCNTs-PLA) are affected by process parameters viz nozzle diameter (0.2 mm, 0.4 mm, 0.6 mm), and infill pattern (triangular, honeycomb, rectilinear) through fused filament fabrication (FFF). Flexural testing was carried out on the fabricated specimens, and post to the testing, fractography has been carried out and statistical analysis of the observations is performed utilizing analysis of variance and Taguchi method. According to the observations, flexural strength of the polymer composite specimen increases with increase in nozzle diameter (ND). The flexural behaviour is also directly impacted with the variation of infill pattern (IP). Process parameter variations affect target factors differently depending on the fabricating material. For flexural behaviour, IP contributes 68.27% to CF-PLA, while ND contributes 88.96% to CF-PETG and 77.59% to MWCNTs-PLA. Overall, the highest flexural strength, 70.372 MPa, is exhibited by the specimen with ND 0.6 mm and rectilinear IP for MWCNTs-PLA as fabricating filament material. This study will aid researchers and designers in developing FFF-fabricated electrochemical energy storage devices with improved flexural behaviour of functional parts for a wide range of applications.
4 February 2023 in Journal of Applied Polymer Science
The emergence of additive manufacturing has enabled scientists to efficiently construct complex geometries, facilitating the development of novel, high-impact energy-absorbing structures suitable for a wide range of industrial applications. The present study conducted flexural and impact test to quantitatively assess the energy absorption capabilities of polymer composites fabricated through fused filament fabrication. Specifically, the polymer composites investigated were multi-walled carbon nanotubes reinforced poly-lactic acid, carbon fibre reinforced poly-ethylene terephthalate glycol, and carbon fibre reinforced poly-lactic acid. The investigation also examined the influence of different infill patterns and nozzle hole diameters on the polymer composites. The investigation depicts that by altering the process parameters, the flexural strength is improved from 21.079 MPa to 70.653 MPa by 235.18%. The experimental study of impact specimens utilising the Izod impact test demonstrates that the rectilinear infill pattern and a nozzle hole diameter of 0.6 mm result in the highest energy absorption of 37.76 kJ/m2 for carbon fibre reinforced poly-lactic acid. The study revealed that the energy absorption of the specimens was significantly influenced by both the independent and interaction effects of process variables. The application of the fused filament fabrication demonstrates an improved energy absorption, making it suitable for manufacturing of vehicle and aircraft components.
8 March 2024 in Journal of Thermoplastic Composite Materials
Additive Manufacturing (AM) techniques, particularly Fused Filament Fabrication (FFF), have revolutionized prototyping and low-volume production. Improving the tensile properties of FFF-printed parts is a primary objective to elevate their functional utility. This study aimed to investigate the effects of annealing time (ATM), annealing temperature (ATP), and nozzle diameter (ND) on the tensile strength (TS) of two commonly used printing materials: Polyethylene Terephthalate Glycol (PETG) and PETG reinforced with carbon fibre (PETG-CF). Samples with varying ND (0.4 mm, 0.6 mm, and 0.8 mm) underwent annealing at ATP of 80°C and 100°C for ATM of 60 min and 120 min, respectively. Subsequent tensile tests were meticulously conducted, and regression models were employed to comprehensively analyse the influence of these control factors on TS. The findings from the tensile tests on annealed specimens revealed substantial improvements in TS for both PETG and PETG-CF materials. Statistical analysis, Taguchi method (TM), and response surface methodology (RSM) indicated that ND exerted a more pronounced impact on TS compared to ATM and ATP. By identifying the optimal control factor combinations for each material, the study pinpointed that the best TS was achieved at 0.8 mm ND, 120 minutes ATM, and 100°C ATP for PETG-CF. The remarkable enhancement in tensile properties for annealed FFF-printed parts underscores the potential of PETG-CF to replace structural metallic components in critical applications within the automotive and aeronautical industries.
23 October 2023 in Journal of Materials Engineering and Performance