In this paper, the fretting wear properties of 20CrMnTi steel, a common material for a rocker bracket, was discussed for the first time after it was suffered carburizing treatment. Subsequently, the fretting wear behaviors of virgin, quenched, and carburized states were studied. The effect of loads (corresponding to different engine power output) and reciprocating frequencies (corresponding to different engine speed) on wear behaviors and mechanisms of carburized specimen were further discussed. The results showed that the coefficient of friction (CoF) and wear volume loss (WVL) of the carburized specimens were significantly lower than that of virgin and quenched states. During the wear test, the surface CoF decreased gradually with the increase of applied load, while the linear correlation trend was not observed with the increase of fretting frequency as it showed an increase first and then a decrease. It was observed that the WVL increased gradually with the increase of load and frequency. With an increase of the load, the wear mechanism gradually deteriorated from the initial adhesive wear to the mixed wear mechanism. When the load was high, the oxidative wear became more severe. However, no significant effect of frequency was observed on the wear mechanism.
17Cr2Ni2MoVNb steel is a new type of gear steel in the automotive industry; the rolling contact fatigue behavior is not well documented. In this study, some microscopic analysis methods (optical microscope (OM), scanning electron microscope (SEM), transmission electron microscope (TEM), X-ray diffractometer (XRD), and energy dispersive X-ray analysis (EDS)) were used to characterize material microstructure and damage surface. In addition, rolling contact fatigue behavior was evaluated by Weibull curve. The results show that the size of austenite grain increased while the quenching temperature increased. Moreover, the samples with a quenching temperature of 1000 °C exhibited the maximum mean life of 7.33 × 105 cycles. In addition, the failure mode of quenched at 900 °C and 1100 °C were delamination, and pitting was the main failure mode of 1000 °C.
Increasing load requirements and harsh operating conditions have worsened the wear of drive shafts in special field vehicles. In this paper, the evolution of the microstructure and fretting wear behaviors of 25CrNi2MoVE torsion shaft steel and their influence on the wear mechanisms were investigated as a function of tempering temperature. The results showed that the coarse grain size, low matrix hardness and non-metallic inclusions in the as-received state lead to a high wear rate and serious adhesive wear. The grain refinement after normalizing and the formed M5C2 carbide and bainite helped to improve the wear resistance and worn surface quality. Low temperature tempering is conducive to further improve the wear resistance of normalized samples, and the wear rate and worn surface roughness are increased gradually after tempering temperature increases. For quenching, although martensite structure can achieve a lower wear rate, the coefficient of friction is much higher; the wear mechanisms are primarily fatigue wear and adhesive wear. Although the adhesive wear degree and worn surface roughness were increased, the optimal anti-wear performances are obtained under tempering at 350 °C with good continuity of the surface oxide film. Excessive tempering temperature will make the softened matrix unable to form a beneficial “third-body wear”.
With the rapid development of the automotive industry in China, the common gear steels no longer meet the high speed and heavy load requirements of the automotive industry. 17Cr2Ni2MoVNb steel is a new type of gear steel in the automotive industry, but the mechanical properties of 17Cr2Ni2MoVNb are not well documented. In this study, the tensile properties and rotary bending fatigue behaviors of 17Cr2Ni2MoVNb were investigated, (quenched at 860 °C and tempered at 180, 400, 620 °C); the microstructures and fracture surface were analyzed using an optical microscope, scanning electron microscopy and transmission electron microscopy. The results show that at higher tempering temperatures, the tissue was denser, and the residual austenite transformed into lower bainite or tempered martensite. Dislocation density reduced while tempering temperature increased. Moreover, the samples with a tempering temperature of 180 °C exhibited the highest tensile strength of 1456 MPa, in addition to fatigue limits of 730, 700 and 600 MPa at temperatures of 180, 400, and 620 °C, respectively.
Due to their design, hollow cavity and filled sodium, hollow head and sodium filled engine valves (HHSVs) have superior performance to traditional solid valves in terms of mass and temperature reduction. This paper presents a new manufacturing method for 42Cr9Si2 steel hollow head and sodium filled valves. An inertia friction welding process parameter optimization was conducted to obtain a suitable process parameter range. The fatigue strength of 42Cr9Si2 steel at elevated temperatures was evaluated by rotating bending fatigue test with material specimens. Performance evaluation tests for real valve components were then carried out using a bespoke bench-top apparatus, as well as a stress evaluation utilizing a finite element method. It was proved that the optimized friction welding parameters of HHSV can achieve good welding quality and performance, and the HHSV specimen successfully survived defined durability tests proving the viability of this new method. The wear resistance of the HHSV specimens was evaluated and the corresponding wear mechanisms were found to be those classically defined in automotive valve wear.