III-V/silicon solar cells which have an active silicon bottom solar cell are promising for multi-junction solar cell applications. In such solar cell structures, a high minority carrier lifetime in the bulk silicon substrate is necessary. Annealing silicon wafers at high temperature (> 500oC) in the molecular beam epitaxy (MBE) high-vacuum chamber revealed significant lifetime degradation. In this work, we developed a practical method to maintain high Si bulk lifetime. SiNx layer deposited on Si back side helps maintain millisecond level minority carrier lifetime. By this procedure high minority carrier lifetime in the Si substrate is preserved while high quality thin GaP layer is achieved. We demonstrate GaP as a hetero-emitter layer with high Si bulk lifetime in GaP/Si structure solar cell with 524mV open circuit voltage.
A major hindrance to the development of devices integrating III-V materials on silicon is the preservation of its electronic quality. In this contribution, we report on the severe decrease in silicon bulk minority-carrier lifetime after heteroepitaxial growth of gallium phosphide, in our molecular beam epitaxy (MBE) system. The drop in lifetime occurs after annealing silicon above 500°C; we assign the increased recombination rate to extrinsic defect originating from highly mobile impurities diffusing from the MBE chamber. We show that the contaminant can be gettered by phosphorous diffusion. We investigate two approaches to protect the Si bulk lifetime by containing the contaminant to a part of the silicon that can be removed by etching. This provides a path to successful III-V growth on silicon.
GaSb and alloys based on the 6.1 Å family can be grown metamorphically on substrates such as GaAs allowing for the realization of several multijunction solar cell designs. This paper investigates the molecular beam epitaxy growth, crystal quality, and device performance of Al$_{\text {x}}$Ga$_{1-}$$_{\text {x}}$Sb-based single-junction solar cells grown on GaAs substrates. The focus is on the optimization of the growth of Al$_{1-}$$_{\text{x}}$Sb on GaAs (001) substrates in order to minimize the threading dislocation density resulting from the large lattice mismatch between GaSb and GaAs. Utilizing optimum growth conditions, solar cells with absorbing layers of different Al$_{\text{x}}$Ga$_{1}$$_{\text {x}}$Sb compositions are studied and compared to control cells grown on lattice-matched GaSb substrates. GaSb, Al$_{0.15}$Ga$_{0.85}$Sb, and Al$_{0.5}$Ga$_{0.5}$Sb solar cells grown on GaAs substrates show open-circuit voltages of 0.16, 0.17, and 0.35 V, respectively. Furthermore, the lattice-mismatched cells demonstrate promising carrier collection with comparable spectral response to lattice-matched control cells grown on GaSb.
We observe a degradation of the minority-carrier lifetime in silicon substrates after a temperature cycle in a molecular beam epitaxy (MBE) chamber that is representative of the growth of III–V materials. This decrease in the lifetime is from milliseconds to microseconds, and in some cases into the sub-microsecond range. The degradation appears to be caused by thermally activated diffusion of metals from the back side of the substrate, occurring at temperatures above 500 °C. This impacts the ability to achieve high-performance monolithic III–V/Si multi-junction solar cells, since the epitaxial growth usually requires high-temperature steps (over 700 °C) for surface de-oxidation or surface reconstruction and temperatures of 400–600 °C during the epitaxial growth. We show that, through phosphorous diffusion gettering, the lifetimes of degraded wafers can be recovered to the millisecond range. Further, we demonstrate that a silicon nitride coating functions both as a diffusion barrier and as an interfacial gettering or hydrogenation agent, enabling high minority-carrier lifetimes directly out of the MBE chamber. This approach allows for the silicon minority-carrier lifetime to be maintained in the millisecond range without the need for post-growth recovery, providing a path to achieve high-efficiency III–V/Si solar cells.