Ti 4 O 7 nanoparticles grown on hollow carbon spheres through the carbothermal reduction reaction exhibit high sulfur loading, superior reversible capacity and favorable cycling stability.
The structures of two types of interfaces between different Ti n O 2n−1 phases have been investigated based on comprehensive XRD and TEM analysis. Combined with thermodynamic calculations, the structural evolutions and formation mechanisms of these interfaces are further proposed in detail.
Crystallography of phase transformation combining transmission electron microscopy (TEM) with in situ heating techniques and X-ray diffraction (XRD) can provide critical information regarding solid-state phase transitions and the transition-induced interfaces in TiO2 nanomaterials theoretically and experimentally. Two types of reduced titanium oxides (Ti3O5, Ti6O11) are found during ex situ and in situ heating of TiO2 (B) nanofibers with a specific morphology of the {100} single form (SF) in air and vacuum. The results indicate that the phase transformation process from TiO2 (B) follows the TiO2 (B) → Ti3O5 → Ti6O11 → anatase sequence for the nanofibers with the {100} SF. The occurrence of such a phase transition is selective to the morphology of TiO2 (B) nanofibers. The corresponding orientation relationships (COR) between the four phases are revealed according to the TEM characterization. Four types of coherent interfaces, following the CORs are also found. They are TiO2 (B)/Ti3O5, TiO2 (B)/Ti6O11, Ti6O11/anatase and TiO2 (B)/anatase respectively. The habit plane for the TiO2 (B) to Ti3O5 transition is calculated as the {100}TB by using the invariant line model. The detailed atomic transformation mechanism is elucidated based on the crystallographic features of the four phases.
Ni–Cu alloy-based nanomaterials are representative cost-effective materials that have been widely used as highly active and stable electrocatalysts for electrochemical energy applications, such as the water oxidation reaction, the methanol/ethanol reaction and many other small molecule oxidation reactions. Here, novel short needle-like complex oxides of NixCu1−x/CuO/Ni(OH)2 are rationally designed and synthesized to further promote their oxygen evolution reaction (OER) performance. Under the tuning of electron perturbation and surface morphology, Ni0.7Cu0.3/CuO/Ni(OH)2 reached an optimum performance of ∼136.6 mVRHE kinetic potential and ∼160 mVRHE (vs. 3.33 A g−1) over-potential with a Tafel slope of 66 mV dec−1. Furthermore, the complex oxides are directly grown on glass carbon, which works as a binder-free and carbon-free electrode, leading to an excellent stability of 200 000 s with 39% activity loss. Due to the electron perturbation role of Cu as well as the synergistic interactions among Ni–Cu, CuO and Ni(OH)2, the obtained Ni0.7Cu0.3/CuO/Ni(OH)2 complex oxide is significantly more active and stable than those of NixCu1−x alloy, CuO and Ni(OH)2. Our results demonstrate a general strategy to design cost-efficient OER electrocatalysts by using a conventional and easily accessible Ni0.7Cu0.3/CuO/Ni(OH)2 hybrids to possibly replace commercial Ru/Ir-based materials.
17 January 2025 in Journal of Materials Chemistry C