10 November 2025 in Metals
Verified
Journal Article
Open access
PDF file
JLJiahua Liu
Jiahua Liu
AZAiquan Zheng
Aiquan Zheng
LWlei wang
lei wang
HXHongwu Xu
Hongwu Xu
FJFeifei Ji
Feifei Ji
JLJiong Luo
Jiong Luo
In this study, the J-integral method was used to evaluate the fracture toughness (JQ) of the isolation layer at the top of SA508-III-309L/308L-316L dissimilar metal welded joints (DMWJs) of a pressure vessel. Tests were carried out at varying temperatures, from room temperature to 320 °C, to study the mechanism underlying temperature effects on unstable crack propagation. The results show that failure occurs in the middle position of the weld isolation layer of the welded joint at all test temperatures. The JQ of the inner diameter of the joint decreases with increased temperature, with a maximum decrease of 31.8%. The analysis shows that the lath ferrite structure in the isolation layer provides a favorable path for crack propagation. The increase in temperature enlarges the difference in thermal expansion between SA508-III steel and the isolation layer, making it easier for second-phase particles in the isolation layer to induce crack initiation and propagation, thus reducing the JQ of the steel. In addition, at high temperatures, the dislocation density of the isolation layer, the deformation resistance of the material, and the difference in the yield ratio of the joint weld all decrease, which is not conducive to the redistribution of the stress field at the tip of the fatigue crack, leading to further reduction in the JQ.

14 March 2026 in Metals
Verified
Journal Article
Open access
PDF file
JLJiahua Liu
Jiahua Liu
AZAiquan Zheng
Aiquan Zheng
LWlei wang
lei wang
HXHongwu Xu
Hongwu Xu
FJFeifei Ji
Feifei Ji
ZJZhiyong Jiang
Zhiyong Jiang
For the failure issue of the weak part of the safety end of the nuclear power pressure vessel connection, the J-integral method was used to test the fracture toughness of the weak part at the bottom of the dissimilar metal welded joints (DMWJs) of SA508-III and 316L in the temperature range of 25 °C to 320 °C, and the mechanism of temperature-induced crack instability and propagation was studied. The research results indicate that at all test temperatures, the position of the weld near the 316L steel is the failure site of the welded joint. The fracture toughness of the joint decreases with increasing temperature, with a maximum decrease of 42.0%. Analysis shows that as the temperature increases, the dislocation density decreases, the tensile strength decreases, and the yield strength ratio decreases, making it easier for secondary cracks to initiate near the crack tip, thereby accelerating the unstable propagation of cracks. At the same time, as the temperature increases, the number of twin crystals that can promote crack turning and prolong the crack propagation path decreases, the energy absorbed before fracture decreases, and the fracture toughness value decreases accordingly, further accelerating the unstable propagation of cracks.