Relevance. Increasing the service life of mining tools is an important task in the development of geology associated with the investigation of new ceramic materials for functional purposes. The ability to reduce wear and thermal and chemical effects of rocks on the working elements of mining equipment determines the vector of development of the use of super-hard, high-strength and refractory ceramics. At the same time, the task is set to increase the fracture toughness of the materials used to solve the problem of maintaining the operability of equipment under conditions of critical deformations. To accomplish this task, it is necessary to study the patterns of consolidation of ceramic materials and search for the optimal combination of consolidation parameters to achieve improved physical and mechanical properties. Aim. To develop a method for producing high-density durable ceramics based on commercially available zirconium nitride powders using spark plasma sintering under vacuum conditions, to study the phase composition and physical and mechanical properties of the resulting samples. Methods. X-ray phase analysis of the studied samples, nanoindentation, microscopic analysis. Results and conclusion. The authors have studied the physical and mechanical properties of zirconium nitride consolidated by spark plasma sintering at 2000℃, a pressure of 30–60 MPa and a holding time at a given temperature of 5–10 minutes. Qualitative and quantitative X-ray phase analysis was carried out, within which the content of the main phase of zirconium nitride and zirconium dioxide phase was determined. It was found that an increase in the pressure applied during consolidation and holding time contributes to better compaction and a decrease in the porosity of the samples from 8.52 to 2.72%. It was found that with a decrease in porosity, the elastic modulus increased in the range from 320 to 378 GPa, and the hardness from 7.3 to 10.4 GPa. At the same time, by extrapolating the data, it was established that non-porous zirconium nitride samples will have an elastic modulus of 394 GPa and a Martens hardness of 11.56 GPa. For the samples under study, critical stress intensity factors were determined. It was established that at a porosity of less than 5%, the critical stress intensity factor of zirconium nitride consolidated by spark plasma sintering has values of at least 4 MPa m1/2.
\mathrm{ZrCN-ZrO_2} ceramics were produced by hot pressing at a temperature of 2273 K, a pressure of 30 MPa, and a holding time at a given temperature of 15 minutes. Sintering was carried out in a vacuum environment. High-density \mathrm{ZrCN-ZrO_2} ceramics were manufactured using zirconium nitride and carbide powders. Zirconium dioxide acted as a sintering additive due to its lowest melting point among the studied compounds. Using scanning electron microscopy and X-ray phase analysis, the presence of zirconium carbonitride as a matrix phase with different stoichiometry, depending on the change in the initial composition of the powders, was established. An increase in strength, hardness, Young''s modulus, and crack resistance of the studied materials was observed with an increase in the content of zirconium nitride in the mixture of initial powders and a decrease in the porosity of the material. At the same time, a decrease in subgrains was recorded according to the results of X-ray phase analysis.