To evaluate the immediate enamel bond strength, in situ degree of conversion and the polymerisation rate of three experimental orthodontic adhesives containing triclosan-loaded halloysite nanotubes. The antibacterial and bioactivity properties of such experimental materials were also assessed. Three experimental orthodontic adhesives were formulated by incorporating triclosan-loaded halloysite nanotubes (TCN-HNT) at different concentrations (5wt%, 10wt% and 20wt%) into a resin blend (Control). The maximum polymerisation rate of the tested adhesives was evaluated trough FTIR, while Raman was used to analyse the in situ degree of conversion (DC) at the bracket/enamel interface. The shear bond strength (SBS) of the enamel-bonded specimens was assessed at 24h. The antibacterial properties of the experimental materials against S. Mutans were evaluate up to 72h, while, their bioactivity was evaluated after 14days of artificial saliva (AS) storage through SEM-EDS and Raman spectromicroscopy. Incorporation of TCN-HNT increased the polymerisation properties without interfering with the immediate bonding properties of the experimental adhesives. All experimental adhesives containing TCN-HNT inhibited bacterial growth at 24h, and induced mineral deposition after 14days of AS storage. At 72h, only the experimental system containing 20% TCN-HNT maintained such a capability. Adhesives doped with TCN-HNT present improved polymerisation properties and suitable bonding performance. However, only the adhesives containing TCN-HNT >10% might promote long-term antibacterial activity and reliable mineral deposition. The use of adhesives containing triclosan-loaded halloysite represents a promising "smart" approach to bond orthodontic brackets and bands; these might prevent enamel demineralisation and induce enamel remineralisation during the treatment.
Orthodontic adhesives with antimicrobial and remineralizing properties may be an alternative to control white spot lesions around brackets. The aim of this study is to develop an experimental orthodontic adhesive containing boron nitride nanotubes (BNNT) and alkyl trimethyl ammonium bromide (ATAB). Methacrylate (BisGMA and TEGDMA) monomers were used to formulate the adhesives. Four experimental groups were produced with the addition of 0.1 wt.% BNNT (GBNNT); 0.1 wt.% ATAB (GATAB); and 0.2 wt.% BNNT with ATAB (GBNNT/ATAB); in the control group, no fillers were added (GCtrl). The degree of conversion, cytotoxicity, softening in solvent, contact angle and free surface energy, antibacterial activity, shear bond strength, and mineral deposition were evaluated. Adhesives achieved degree of conversion higher than 50% and cell viability higher than 90%. GBNNT and GATAB adhesives exhibited reduced softening in solvent. Mean free surface energy was decreased in the GBNNT adhesive. Significant reduction in bacterial growth was observed in the GBNNT/ATAB. No statistical difference was found for shear bond strength. Mineral deposition was found in GBNNT, GATAB, and GBNNT/ATAB groups after 14 and 28 days. The addition of 0.2% BNNT/ATAB to an experimental orthodontic adhesive inhibited bacterial growth and induced mineral deposition without affecting the properties of the material.