Considering the necessity for a biodegradable implant alloy with good biocompatibility and mechanical strength, dual ceramic particles of HAP and Al2O3 were added to Mg-Zn alloy to produce a new hybrid composite using powder metallurgy. The paper reports the mechanical and corrosion behaviour of Mg-Zn/HAP/Al2O3 hybrid composites containing variable wt.% HAP and Al2O3 with 15 wt.% total ceramic content. The powders of Mg, Zn, Al2O3 and HAP were milled in a high-energy ball mill, and then compacted under 400 MPa and sintered at 300 °C. Density and compression strength increased with increasing Al2O3 content. HAP facilitated weight gain in Hanks balanced salt solution due to deposition of an apatite layer which promoted anodic behaviour with higher corrosion resistance. A hybrid composite of Mg alloy with 5 wt.% Al2O3 and 10 wt.% HAP displayed 153 MPa compressive strength, 1.37 mm/year corrosion resistance and bioactivity with a CA:P ratio of 1:1.55 and appears to be the most promising biodegradable implant material tested.
1 June 2017 in IOP Conference Series: Materials Science and Engineering
There are many examples of organic coatings used for corrosion protection. In particular, hydrophobic and super-hydrophobic coatings are shown to give good protection because of their enhanced ability to slow down transport of water and ions through the coating. The purpose of this research is to develop water repellent coating to avoid direct contact between metal and environment corrosive and mitigate corrosion attack at pipeline system. This water repellent characteristic on super-hydrophobic coating was coated by electrodeposition method. Wettability of carbon steel with super-hydrophobic coating (cerium chloride and myristic acid) and oxidized surface was investigated through contact angle and inhibitor performance test. The inhibitor performance was studied in 25% tannin acid corrosion test at 30°C and 3.5% sodium chloride (NaCl). The water contact angle test was determined by placing a 4-μL water droplet of distilled water. It shows that the wettability of contact angle super-hydrophobic with an angle of 151.60° at zero minute can be classified as superhydrophobic characteristic. By added tannin acid as inhibitor the corrosion protection on carbon steel becomes more consistent. This reveals that the ability of the coating to withstand with the corrosion attack in the seawater at different period of immersions. The results elucidate that the weight loss increased as the time of exposure increased. However, the corrosion rates for uncoated carbon steel is high compared to coated carbon steel. As a conclusion, from both samples it can be seen that the coated carbon steel has less corrosion rated compared to uncoated carbon steel and addition of inhibitor to the seawater provides more protection to resist corrosion attack on carbon steel.
Initial solution treatment (ST) of aluminium alloys prior cryorolling (CR) enhances the ultrafine grain structure formation hence, improving their mechanical and corrosion properties. However, determining the appropriate ST temperature is crucial to obtain the optimum properties. In this work, ST followed by cryorolling of AA 5052 alloy was performed at varying temperatures; 480 °C, 510 °C and 540 °C. Mechanical and microstructural characterization of the cryorolled samples with and without ST and the base metal were performed using Vickers hardness tester, universal tensile testing machine, FESEM, EBSD and HRTEM. All the ST cryorolled samples showed the finer structure and better mechanical and corrosion performances than those without ST and the base metal. The smallest crystallite size and lattice strain achieved were 24.88 nm and 3.86 × 10−3 respectively at 540 °C. The hardness, yield and tensile strength increased with increasing the ST temperature with the highest values of 85.2 Hv, 254.82 MPa and 303.35 MPa, respectively, at 540 °C. Cryorolled sample solution treated at 540 °C also showed the highest corrosion resistance based on low corrosion current and high corrosion potential. The work gives the appropriate ST temperature at which improved microstructure, mechanical and corrosion properties of the cryorolled AA5052 can be obtained.
31 October 2014 in Applied Mechanics and Materials
Tungsten carbides (WC) are widely used as wear resistant components such as seal, valves, rings, nozzle and bearings. But in some processing operations, the environment necessarily includes severe corrosion or extremes of temperatures. In paper reveal, the corrosion performance of commercial cobalt tungsten carbide (WC-6%Co) and nickel tungsten carbide (WC-9%Ni) in seawater with 3.5% salinity. The experiment was performed in four different temperatures (20°C, 40°C, 60°C and 80°C) and the surface structure by corrosion attack was reveal under SEM. The Icorr value of WC-9%Ni is lower than WC-6%Co, elucidate that WC-9%Ni is better in corrosion resistance compare to WC-6%Co. As the temperature increased, the corrosion rate for every material increased as expected. Decreasing in hardness value for both materials reveal that, the material’s hardness decrease after corrosion has attacked.
30 October 2017 in Journal of Physics: Conference Series
Porous metals also known as metal foams is a metallic body having spaces orpores through which liquid or air may pass. Porous metals get an attention from researchers nowadays due to their unique combination of properties includes excellent mechanical and electrical, high energy absorption, good thermal and sound insulation and water and gas permeability. Porous metals have been applied in numerous applications such as in automotive, aerospace and also in biomedical applications. This research reveals the influence of corrosion attack in porous austenitic stainless steel 316L. The cyclic polarization potential analysis was performed on the porous austenitic stainless steel 316L in 3.5% NaCl solution. The morphology and the element presence on the samples before and after corrosion attack was examined using scanning electron microscopy (SEM) and energy dispersive x-ray (EDX) respectively to determine the corrosion mechanism structure. The cyclic polarization potential analysis showed the result of (Ecorr) for porous austenitic stainless steel type 316L in the range of -0.40v to -0.60v and breakdown potential (Eb) is -0.3v to -0.4v in NaCl solution.
31 October 2014 in Applied Mechanics and Materials
Cyclic polarization test was used to determine the breakdown potential of passive film for stainless steel 316L at different temperatures (20°C, 30°C, 40°C, 50 °C) and different salinity (15%, 25%, and 35%). The results show the highest breakdown potential occur at low temperature and low salinity indicate that incresing the temperature and salt content in seawater will increasing the corrosion attack on 316L. Increasing the temperature from 20°C to 50°C was decrease the Eb value for 75%. Before and after testing, visible pits and hardness for each sample were observed by using Scanning Electron Microscopy (SEM) and Vickers hardness testing. It was found that at temperature 20°C, it can be seen that number of pits is more but the pits size is a bit tiny. However, the number of pits reduce as the temperature and salinity increased but the size of the pit become larger and wide which indicate that pitting has propagate during that period. Furthermore, increasing the temperature from 20°C to 50°C also lead to increased the hardness different value which indicate that reducing in hardness properties of 316L at increasing salinity because of corrosion attack.