Epitaxial ZnSe/epitaxial GaAs interfaces have been grown using molecular beam epitaxy and evaluated by capacitance–voltage measurements and transmission electron microscopy. The GaAs surface stoichiometry was systematically varied prior to the nucleation of ZnSe. A significant reduction of interface state density occurred when the GaAs epilayer surface was As deficient. The resulting interface state densities of as-grown structures are comparable to values obtained with (Al,Ga)As/GaAs interfaces.
A series of three-dimensional morphology changes of fine eutectic Si-particles during heat treatment have been investigated in Self-modified and Sr-modified Al-10%Si cast alloys by means of synchrotron radiation nanotomography utilizing a Fresnel zone plate and a Zernike phase plate in this study. The coral-like shape particles observed in Sr-modified cast alloy fragmented at branch and neck during heat treatment at 773 K. The fragmentation occurred up to 900 s. After that, the fragmented particles grew and spheroidized by Ostwald ripening. On the other hand, rod-like shaped eutectic Si-particles observed in self-modified cast alloy were larger in size compared with the particle size in Sr-modified cast alloy. Separation of eutectic Si-particles in Self-modified cast alloy occurred up to approximately 900 s, which was similar tendency to that in Sr-modified cast alloy. However, it was found that the morphology change behavior was very complex in rod-like shape Si-particles. The three-dimensional morphology changes of fine eutectic Si-particles in both cast alloys, specifically fragmentation and spheroidizing, can be connected to changes in mechanical properties.
In welded maraging steels, mechanical properties, particularly ductility and toughness, are often compromised in the heat-affected zone (HAZ). This study focuses on 300-grade maraging steel bars, solution annealed at 1123 K for 1.5 h (5.4 ks) and welded using gas tungsten arc welding, followed by a post-weld heat treatment at 753 K for 13.33 h (48 ks). In situ observations during three-point bending tests on HAZ samples featuring coarsened prior austenite grain sizes were conducted to examine damage behavior and the crack path near the crack tip. The main crack initiated at the peak applied load during the bending test and, upon further loading, exhibited significant deflection and extension accompanied by numerous microcracks and localized crack branching. Distinctive damage features, such as transgranular cracking across block regions, intense intergranular cracking along packet boundaries with a pronounced shear component, and crowding of microcracks ahead of the crack tip, were observed in the HAZ sample during the in situ test. The interaction between the main crack tip and microcracks and its influence on the local crack propagation driving force was discussed using fracture mechanics. Experimental results, including tensile fracture surface observations and in situ images, along with analysis of the stress anti-shielding effect by microcracks, suggest that the HAZ sample exhibits embrittlement fracture behavior with lower ductility and toughness compared to the base metal sample.