The top-seeded infiltration growth process (TSIG) is one of the most important methods for the fabrication of single-domain rare-earth barium copper oxide (REBCO) bulk superconductors. The performance of samples is in the main closely related to the quality of the solid phase pellets (SPPs). In this paper, we report a new method for optimizing the SPPs and properties of single-domain REBCO bulks, including sintering of the SPPs (Y2O3 + BaCuO2), infiltration of the Ba–Cu–O liquid phase and the melting growth process. A group of single-domain YBCO bulk superconductors with a diameter of 20 mm have been fabricated by the modified RE + 011 TSIG method. Both the levitation force and the trapped field of the samples increase at first and then decrease with increase in the sintering time. The largest levitation force of 42.8 N and trapped field of 0.41 T (77 K, 0.5 T) are obtained in the sample sintered at 1000 °C for 4.5 h; this is mainly related to the optimal microstructure of the pre-sintered SPPs and the YBCO bulk. These results indicate that pre-sintering and high-temperature infiltration is a very important method for controlling the microstructure and improving the physical properties of single-domain YBCO bulk superconductors.
In this study, the effect of the pre-infiltration temperature (Ti) on the liquid-phase infiltration characteristics and its effect on the magnetic properties of single-domain GdBCO bulks prepared by the top-seeded infiltration growth (TSIG) method are comprehensively investigated. The results reveal that (1) the liquid Ba-Cu-O phase (LP) did not uniformly infiltrate into the Gd2BaCuO5 (Gd-211) solid-phase pellet (SPP). (2) The initial melting and infiltration of the LP occurred at approximately 920 °C. The average infiltration depth and amount of LP that infiltrated the SPP increased with increasing Ti accompanied by the shrinkage and depletion of the LP pellet. (3) The LP penetrated up to the top surface of the SPP and uniformly infiltrated throughout the SPP when the Ti was approximately 960 °C and 1020 °C, respectively. (4) The mean Gd-211 particle size of the pre-infiltrated SPP increased from 1.94 µm at 920 °C to 2.52 µm at 1040 °C as the Ti rose. (5) The magnetic properties and microstructure of the single-domain GdBCO bulks were significantly influenced by the microstructure of the pre-infiltrated SPP. The largest levitation force of 35.64 N and trapped field of 0.23 T were obtained in the single-domain GdBCO bulks at an infiltration Ti of 960 °C.