Carbon fiber-reinforced composite (CFRC) is a well-known hi-tech material with diverse applications. The CFRC faces several environmental conditions during its application, e.g., elevated temperatures, humidity, exposure to UV radiation, and acidic and alkaline environments. These environmental factors strongly affect the performance of CFRC, and they tend to age with time. Aging reduces the mechanical properties of the composite and ultimately its service life. In this review, the focus is on the aging of composite, common types of aging (thermal, hydrothermal acid and alkaline, and UV radiation), and the role of the third phase (fillers) in the aging process. There are numerous factors involved in the aging of composite. Aging starts with microcracks and proceeds towards delamination which further exposes the internal surface to environments. When the depths are exposed, free radicals are released and further deteriorate the internal structures. They create more pathways for oxygen to reach every millimeter of composite, thus reducing the mechanical performance of the composite. Usually, a trend is seen that introducing filler might slow down or compensate for the mechanical performance after aging. This trend is explored in the review article. However, usually, the third phase remained neutral and sometimes reduced and/or enhanced the mechanical properties after aging. In thermal aging, different metallic oxides have a noteworthy effect on mechanical performance. The synergistic effect of the third phase and aging on CFRC mechanical performance is also tabulated.
Aluminium alloy foam is a lightweight material with high energy absorption properties and can potentially replace bulk Al-components. The aim of this work is to develop a brazing technique to join aluminium facing sheets to aluminium alloy foam to obtain aluminium foam sandwich panels for applications where high service temperature is a requirement. Al-6016 alloy sheets were brazed to aluminium alloy foam using two aluminium based (Al-Cu-Mg and Al-Si-Mg-Ti) metal glasses at 560 °C–590 °C in an argon atmosphere. Microstructure and microhardness profiles of the aluminium alloy sheet/aluminium alloy foam brazed joints were analysed using a microhardness tester and scanning electron microscope equipped with electron dispersion spectroscopy. A three-point bending test was conducted to study the flexural behaviour of the aluminium foam sandwich composite panels.
In aerospace and automotive applications, composite materials are used as a major structural material along with metals. Composite-metal and metal-metal joining are very crucial in such structures. Adhesive bonding is commonly used for this purpose. Since such structures are exposed to varying temperatures and dynamic loads, it is essential to investigate the response of such joints under thermomechanical loading. Though various studies have been reported in the literature to assess the thermomechanical properties of composites, adhesives, and their joints, the effect of the surface treatment of metals and composites on the improvement in the thermomechanical behavior of the joints has not been reported. The metal and composite surfaces were modified using chemical etching techniques. The interaction between adhesives and adherends was studied using the DTMA technique in compression mode. Anodizing treatment on aluminum alloys improved the stiffness properties of metallic joints to 36% and decreased the damping to 23%, while chemical treatment on composite and metal adherends increased the stiffness of composite-metal joints to 34% and reduced the energy dissipation to 20%.
This chapter explores the innovative field of multicomponent composites, focusing on three distinct yet interconnected areas: biobased composites, elastomeric composites, and membranes. The first section delves into biobased multicomponent composites, highlighting the use of renewable resources to create sustainable materials that reduce environmental impact. These composites combine natural fibers with biopolymers, enhancing mechanical properties while promoting eco-friendliness. In the second part, the chapter examines multicomponent elastomeric composites, which leverage the unique properties of elastomers for applications requiring flexibility and resilience. The discussion includes the design strategies employed to optimize performance and durability through the integration of various components. The final section addresses multicomponent membranes, emphasizing their critical role in filtration and separation technologies. The chapter details the fabrication methods and performance characteristics of these membranes, showcasing their potential in diverse applications such as water purification and gas separation. Overall, this chapter provides a comprehensive overview of the advancements in multicomponent composites, illustrating their versatility and importance in addressing contemporary material challenges. <!----> <!----> <!----> <!---->