Superconductivity in nanostructured ceramics offers significant advantages over the conventional coarse-grained materials in view of miniaturization of superconducting electronic devices. In this paper, we report the formation of four morphologies of superconducting YBa2Cu3O7-δ (YBCO) nanostructures by electrospinning technique using polymeric polyvinyl pyrrolidone (PVP) solutions of different molecular weight and altering the total content of the metallic precursors. The morphologies prepared using this strategy are nanorods (NRs), nanogarlands (NGs), nanohierarchical (NH), and nanoparticles (NPs). Alternating current susceptibility measurements showed high critical temperatures (TC ~90 K) for the NH YBCO synthesized using PVP of the lowest molecular weight; whereas the YBCO NRs synthesized using a higher molecular weight polymer showed the lowest TC (82 K). A relationship between the particulate properties and TC was also observed – the lower is the pore size the higher is the TC. The YBCO NGs showed the highest specific surface area (7.06 m2/g) with intermediate TC (88 K). Electrospinning process appears an effective and controllable technique to produce different nanomorphologies with intrinsic properties suitable for practical applications.
The effect of anealing temperature on structural properties of Lanthanum Iron Garnet (LIG) nanofiber has been studied. The LIG nanofiber were prepared by electrospinning technique. This technique has been extensively developed as a simple and efficient method for drawing nanofibers from polymer solutions. The viscous LIG solution were loaded in syringe and were pumped at 0.05 mL/h. The nanofibers were collected on aluminium foil and were treated at 700 °C, 750 °C and 1000 °C in order to study the effect of annealing temperature to the nanofibers structure. X-Ray Diffraction (XRD) and Field Emission Scanning Electron Microscope (FESEM) were employed to study the phase formation and morphology of the samples. The XRD results of LIG nanofiber reveals that as the annealing temperature increases from 700 °C to 1000 °C, the corresponding peaks become sharper and narrower, which demonstrate the improvement of crystallinity and crystallite size. The FESEM images of LIG nanofiber demonstrates that the nanofibers treated at 700 °C have continuous structure with a relatively rough surface and their diameter range is within 41.3 nm and 58.7 nm. Subsequently, when the calcination temperature increase further, the morphology of the sample is dramatically changed. As calcinations temperature rises to 750 °C, the surface of resultant nanofibers start to become agglomerate due to the growth and coalescence of the particle in the nanofibers under the calcination process and the nanofibers structure change back to continuous structure with bigger diameter at 1000 °C as compared to calcination temperature of 700 °C.