Tthe present work studied the cationic substitution of Y3+ by Bi3+ on the crystal structure of orthorhombic YFeO3 and its effect over magnetic, dielectric and electric properties of multiferroic yttrium orthoferrite. Stoichiometric mixtures of Y2O3, Fe2O3 and Bi2O3 were mixed and milled for 5 h using a ball to powder weight ratio of 10:1 by high-energy ball milling. The obtained powders were pressed at 1500 MPa and sintered at 700 °C for 2 h. The test samples were characterized at room temperature by X-ray diffraction (XRD), vibrating sample magnetometer (VSM), scanning electron microscope (SEM), energy dispersive X-ray spectroscopy (EDS) and impedance spectroscopy (IS). The X-ray diffraction patterns disclosed a maximum solubility of 30 % mol. of Bi3+ into the orthorhombic YFeO3. For higher concentrations, a transformation from orthorhombic to garnet structure was produced, obtaining partially Y3Fe5O12 phase. The substitution of Bi3+ in Y3+ sites promoted a distortion into the orthorhombic structure and modified Fe-O-Fe angles and octahedral tilt. In addition, it promoted a ferromagnetic (FM) order, which was attributed to both the crystal distortion and Dzyaloshinskii-Moriya interaction. For doped samples, an increase in real permittivity values was observed, and reduced with the increase of frequency. This in good agreement with the Maxwell-Wagner effect.
We present the synthesis of M-type strontium hexaferrite by sonochemistry and annealing. The effects of the sonication time and thermal energy on the crystal structure and magnetic properties of the obtained powders are presented. Strontium hexagonal ferrite (SrFe12O19) was successfully prepared by the ultrasonic cavitation (sonochemistry) of a complexed polyol solution of metallic acetates and diethylene glycol. The obtained materials were subsequently annealed at temperatures from 300 to 900 °C. X-ray diffraction analysis shows that the sonochemical process yields an amorphous phase containing Fe(3+), Fe(2+) and Sr(2+) ions. This amorphous phase transforms into an intermediate phase of maghemite (γ-Fe2O3) at 300 °C. At 500 °C, the intermediate species is converted to hematite (α-Fe2O3) by a topotactic transition. The final product of strontium hexaferrite (SrFe12O19) is generated at 800 °C. The obtained strontium hexaferrite shows a magnetization of 62.3 emu/g, which is consistent with pure hexaferrite obtained by other methods, and a coercivity of 6.25 kOe, which is higher than expected for this hexaferrite. The powder morphology is composed of aggregates of rounded particles with an average particle size of 60 nm.