The properties of soft–hard interbedded rock masses are significantly impacted by the strength of rock layers and the characteristics of interface surfaces. This study investigates the mechanical properties of soft–hard interlayered rock masses by preparing rock‐like specimens with different interface angles. Uniaxial and triaxial compression tests were conducted to examine the compression mechanical characteristics of the specimens. Experimental results demonstrated that in the uniaxial compression tests, the peak strength of the two‐layer rock‐like specimen exhibits an initial decrease followed by an increase as the interface angle increases. Similarly, the peak strength of the three‐layer rock‐like specimen also follows a “U‐shaped” pattern. The failure of both specimens shifts from tensile failure to shear failure. In the triaxial tests, the strength of the two‐layer rock‐like specimen initially increases and subsequently decreases as the interface angle increases. In contrast, the intensity of the three‐layer rock‐like specimen exhibits a decreasing trend, transitioning from shear dilation or tensile failure to shear failure. By utilizing the damage constitutive model to compute the compressive strength of the composite specimen, it was observed that the deviation from the experimental value did not exceed 2.5%, and the overall shape of the curves was in good agreement. Consequently, it is affirmed that the damage constitutive model developed in this study can accurately capture the pre‐peak phase of the stress–strain relationship in soft–hard interlayered rock‐like specimens, thus providing a valid representation of their mechanical behavior.
7 November 2017 in Geotechnical and Geological Engineering
For the cement‐clay slurry commonly used in dynamic water grouting, consider adding coal ash to optimize the performance of cement‐clay slag composite slurry and discuss the reaction mechanism of the slurry through microchemical element analysis; the orthogonal test was used to study the influence of various factors on material setting time, solidification ratio, water segregation rate, and the optimized ratio of the slurry that was obtained by integrating the unconfined compressive strength of grouting concretion body and slurry configuration cost. The results showed that the water‐solid ratio had the greatest influence on the comprehensive performance, followed by the amount of coal ash admixture. The best performance of the composite slurry was obtained with a water‐solid ratio of 0.8:1 and a cement:coal ash:clay:quicklime:sodium sulfate:water mass ratio of 1:0.45:0.20:0.05:0.07:1.32. Finally, by comparing the mechanical properties of the optimized slurry and the grouting concretion body, it is proved that the optimized slurry has superior performance to meet the general grouting project requirement.
31 March 2017 in The Open Construction & Building Technology Journal
Coal mining is vulnerable to multiple kinds of threat from water incursion. Many coal seams contain dissolved H2S, which may be released during mining, seriously endangering the health of workers. Orthogonal testing was used to analyze the physical and mechanical properties of composite slurries in different proportions. The results showed slurry with a water-solid ratio of 0.8:1 to have the optimal combination of properties. A uniform experimental method was used to investigate the impact of the water-cement ratio, concentration of sodium silicate, and volume of cement-sodium silicate (CS) on the setting time and consolidating strength of CS slurry. This paper provides the appropriate application scope of two grouting materials (optimized composite slurry and CS slurry), based on experimental data and the results of a large number of in situ trials. Finally, the optimized composite slurry and cement-sodium silicate slurry were used to carry out grouting of the center auxiliary transport roadway of the 3−1 coal seam at the Ningtiaota Coal Mine, operated by the Shaanxi Coal Industry Group. It was shown that the type and formula of the slurry could be changed in a timely manner, based on the water outlet and concentration of H2S at the site, achieving successful grouting reinforcement and seepage-proofing.
After water gushing occurs in a coal mine roadway, abundant aggregate needs to be perfused into the water gush roadway to establish a water interception section and reduce the current velocity. Clarifying the water-intercepting aggregate motion path and quantitatively calculating the displacement distance are critical for determining perfusion hole spacing. This paper employs the CFD-DEM coupling approach, which is capable of accurately characterizing the water gush continuous flow properties and the aggregate discrete motion behavior. This can be used to simulate and analyze the water-intercepting aggregate motion in a water gush roadway, categorizing it into three phases: free fall, curvilinear projectile, and sliding. The theoretical motion model aggregate can be developed, and the calculation formulas for aggregate motion distances in each phase derived. A parameter test scheme was designed and combined with numerical simulation methods to verify the accuracy of the formulas. Finally, based on this research, it is proposed that the theoretical model can be used to dynamically optimize the design of perfusion hole spacing, maximizing the synergistic effect of multi-hole perfusion. The selection of aggregate density and size should ensure the vector sum of the aggregate motion distance in phase II and III approaches zero, thereby improving the water-intercepting efficiency.