Diamond-like carbon (DLC) films were prepared from a hydrocarbon precursor gas by plasma source ion implantation (PSII), in which the plasma generation and the film deposition were coupled; i.e., the plasma was generated by the applied voltage and no additional plasma source was used. Several experimental parameters of the PSII process were varied, including the sample bias (high voltage, DC or pulsed), gas pressure, sample holder type and addition of argon in the plasma gas. The influence of the deposition conditions on the carbon bonding and the hydrogen content of the films was then determined using Raman spectroscopy. Nanoindentation was used to determine the hardness of the samples, and a ball-on-disk test to investigate the friction coefficient. Results suggest that films with a lower sp2 content have both a higher hydrogen content and a higher hardness. This counterintuitive finding demonstrated that the carbon bonding is more important to hardness than the reported hydrogen concentration. The highest hardness obtained was 22.4 GPa. With the exception of a few films prepared using a pulsed voltage, all conditions gave DLC films having similarly low friction coefficients, down to 0.049.
The intrinsic high electrical resistivity of diamond-like carbon (DLC) films prevents their use in certain applications. The addition of metal or nitrogen during the preparation of the DLC films leads to a lower resistivity of the films, but it is usually accompanied by several disadvantages, such as a potential contamination risk for surfaces in contact with the film, a limited area that can be coated, deteriorated mechanical properties or low deposition rates of the films. To avoid these problems, DLC films have been prepared by plasma source ion implantation using aniline as a precursor gas, either in pure form or mixed with acetylene. The nitrogen from the precursor aniline is incorporated into the DLC films, leading to a reduced electrical resistivity. Film properties such as hardness, surface roughness and friction coefficient are nearly unchanged as compared to an additionally prepared reference sample, which was deposited using only pure acetylene as precursor gas.
Amorphous carbon films with a high hardness usually suffer from high internal stress. To deposit films with a hard top surface but reduced internal stress, a simple bilayer approach was used. Films were prepared by plasma source ion implantation, using only hydrocarbon precursors. The single layer with the highest hardness (deposited by a low direct current (DC) voltage and radio frequency (RF) generation of the plasma) has the highest internal stress with more than 3.5 GPa. By adding an interlayer with a lower hardness, the resulting stress of the bilayer film can be reduced to below 1.4 GPa while maintaining the high hardness of the top layer. By avoiding metallic interlayers or dopants within the films, the deposition process can be kept simple and cost-effective, and it is also suitable for three-dimensional samples.
A diamond-like carbon (DLC) film with a nanostructured surface can be produced in a two-step process. At first, a metal-containing DLC film is deposited. Here, the combination of plasma source ion implantation using a hydrocarbon gas and magnetron sputtering of a zinc target was used. Next, the metal particles within the surface are dissolved by an etchant (HNO3:H2O solution in this case). Since Zn particles in the surface of Zn-DLC films have a diameter of 100–200 nm, the resulting surface structures possess the same dimensions, thus covering a range that is accessible neither by mask deposition techniques nor by etching of other metal-containing DLC films, such as Cu-DLC. The surface morphology of the etched Zn-DLC films depends on the initial metal content of the film. With a low zinc concentration of about 10 at.%, separate holes are produced within the surface. Higher zinc concentrations (40 at.% or above) lead to a surface with an intrinsic roughness.
The sputter rate influences the resulting thickness of the carbon containing layer within a surface that was treated by plasma immersion ion implantation. Choosing a polycrystalline substrate with rather large crystals and a material with an inherent high sputter rate, inhomogeneous distributions of carbon over the substrate area due to different thicknesses of the incorporated carbon can be detected. A correlation of three factors namely the carbon x-ray intensity in electron probe microanalysis, the thickness of the carbon layer, and the sputter rate in depth profiling measurements via secondary ion mass spectrometry can be shown. Essential for these factors is the crystal orientation that is visualized by mapping via electron backscatter diffraction. The differences in carbon content due to the orientation are most likely one of the reasons that the adhesion of diamond-like carbon films on copper does not improve with an interlayer of implanted carbon.