The microstructures and oxidation behavior of the NbSiTiAlHf alloys doped with rare earth elements at 1300 °C were investigated. The nominal compositions of the selected alloys are Nb-13.5Si-23Ti-37Al-5Hf-0.5X (at.%), where X = Y, Dy, and La, respectively. It was shown that the whole scales were mainly composed of the major phases of Al2O3 and the minor phases of TiO2, where the TiO2 formed on the surface or in the upper layer of scales, for the undoped, Y, and Dy-doped alloy. But, for the 0.5 at.% La-doped alloys, the whole scales were constituted with the major phases of both Al2O3 and TiO2, and contained plenty of large voids. The 0.5 at.% Dy-doped alloys exhibited the lowest scale growth rate with the value of 1.87 × 10−11 cm2/s, and the benefits of Y on the oxidation rates were short-term, while 0.5 at.% La-doped alloys had the highest scale growth rate of 4.55 × 10−10 cm2/s compared with those of all the selected alloys. Then, the effects of Y, Dy, and La on the oxidation behavior of the alumina-scale-forming NbSiTiAlHf alloys were discussed.
Pulsed detonation–plasma technology (PDT) is a surface-modification technology used in an atmospheric environment, where plasma, a detonation impact and thermal conditions are combined and have an effect on the material’s surface. In this study, annealed 65Mn steel was selected to further study the principle of PDT modification. The results show that the modified layer with fine grains was divided into an infiltration layer with a large amount of non-uniformly distributed granular CW3 carbides and a heat-affected layer below the infiltration layer after PDT treatment. However, a higher amount of acicular martensite and a lower amount of austenite was achieved in the modified layer, containing a large number of small-angle grain boundaries, dislocations, and twin grains. After the PDT treatment, the hardness of the modified layer, heat-affected layer, and substrate was 980 HV, 856.2 HV, and 250 HV, respectively. The mass loss of the sample before and after PDT treatment was 21.1 mg and 12.4 mg, respectively. The hardness and wear resistance of the modified layer were greatly improved compared with the substrate because of the combined effect of the solid-phase transformation, element infiltration, and distortion.