As high entropy alloys (HEAs) continue to be increasingly studied for next-generation structural materials, gaining a comprehensive understanding of their mechanical properties, including their creep behaviors, remains essential. In this work, rare earth element yttrium (Y) added CoCrFeNi HEAs are produced by mechanical alloying, followed by consolidation via spark plasma sintering (SPS) with ultrafine grain sizes. The microstructures after SPS consolidation are examined using X-ray diffraction (XRD) and transmission electron microscopy (TEM). The creep properties, including creep displacement, creep strain rate, creep stress, and stress exponent, are evaluated using a nanoindentation test with a Berkovich tip indenter. The results reveal that the average grain size of CoCrFeNi HEA is determined to be 385 ± 65 nm after SPS consolidation, which reduces to 190 ± 30 nm and 155 ± 55 nm with 1 and 4 at.% Y additions, respectively. Accordingly, HEA with the addition of 4 at.% Y exhibits increased hardness, attributed to the presence of additional Y-based oxides and the reduced grain size in its microstructure. Furthermore, the creep mechanisms for the investigated CoCrFeNi HEAs are primarily dominated by dislocation–precipitation interaction based on the calculated stress exponent values.
This study was conducted to understand the creep behavior of two oxide dispersion strengthened alloys containing Zr as the alloying addition by performing indentation creep tests at room temperature. The oxide dispersion strengthened alloys were Fe–8Ni–xZr (x = 1 and 4 at.%, i.e., Zr-1 and Zr-4 alloys, respectively), which had been previously fabricated by mechanical alloying; followed by consolidation via equal channel angular extrusion at 1000 °C. The indentation tests were conducted under a maximum load of 100 mN with the loading rates at 300 and 400 mN min−1. The hardness was calculated by the Oliver–Pharr method, and the creep properties, such as the creep displacement, creep strain rate, creep stress, and stress exponent n, were determined. The results showed that the Zr-4 alloy was harder than the Zr-1 alloy. However, the creep resistance of the Zr-1 alloy was better than that of the Zr-4 alloy. It was further demonstrated that both the hardness and creep resistance depended on the loading rate. Moreover, a possible creep mechanism was proposed. Although the tests were performed at room temperature, they can provide insight into the effect of an oxide dispersion strengthened alloys microstructure on creep at higher temperatures.
CoCrFeNi high entropy alloys (HEAs) with yttrium (Y) additions (1 and 4 at. %) were nanostructured by mechanical alloying process and annealed at various temperatures between 500 °C and 1100 °C. The structure, grain growth, and hardness were studied as a function of solute addition and annealing temperature using X-ray diffraction (XRD), focused ion beam (FIB), and scanning transmission electron microscope (S/TEM) techniques, and hardness test. The thermo-physical calculations were utilized to discuss the phase evolution after mechanical alloying and annealing with respect to added solutes. The results showed that Y additions did not affect the main crystal structure of the base CoCrFeNi HEA as the solid solution with a single face-centered cubic (fcc) crystal structure was maintained even after 1 h annealing at 1100 °C. The as-milled nanocrystalline grain size of CoCrFeNi HEA yielded extensive grain growth with the temperature exposures reaching 291 nm and 1.4 µm after annealing at 900 °C and 1100 °C, respectively. However, Y additions retarded the grain growth and decreased the average grain size upon annealing as compared to the base HEA. That is, 1 and 4 at. % Y additions stabilized the grain size around 88 nm and 95 nm (both determined by TEM) after annealing at 900 °C and 1100 °C, respectively. Accordingly, the as-milled hardness of CoCrFeNi HEA dropped from 475 HV to 220 HV after annealing at 1100 °C, while the reduction in hardness was relatively gradual with Y additions and retained around 435 HV with 4 at. % Y addition even after annealing at 1100 °C. Such thermal stability may facilitate the use of HEAs at high temperatures and enable the consolidation routes of powders into dense nanocrystalline compact HEAs.