High demand of semiconductor gas sensor works at low operating temperature to as low as 100 °C has led to the fabrication of gas sensor based on TiO2 nanoparticles. A sensing film of gas sensor was prepared by mixing the sensing material, TiO2 (P25) and glass powder, and B2O3 with organic binder. The sensing film was annealed at temperature of 500 °C in 30 min. The morphological and structural properties of the sensing film were characterized by field emission scanning electron microscopy (FESEM), energy-dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD). The gas sensor was exposed to hydrogen with concentration of 100–1000 ppm and was tested at different operating temperatures which are 100 °C, 200 °C, and 300 °C to find the optimum operating temperature for producing the highest sensitivity. The gas sensor exhibited p-type conductivity based on decreased current when exposed to hydrogen. The gas sensor showed capability in sensing low concentration of hydrogen to as low as 100 ppm at 100 °C.
This study presents the utilization of mill scale waste, which has attracted much attention due to its high content of magnetite (Fe3O4). This work focuses on the extraction of Fe3O4 from mill scale waste via magnetic separation, and ball milling was used to fabricate a microwave absorber. The extracted magnetic powder was ground-milled using two different techniques: (i) a conventional milling technique (CM) and (ii) mechanical alloying (MM) process. The Fe3O4/CM samples were prepared by a conventional milling process using steel pot ball milling, while the Fe3O4/MM samples were prepared using a high-energy ball milling (HEBM) method. The effect of milling time on the structural, phase composition, and electromagnetic properties were examined using X-ray diffraction (XRD) and a vector network analyzer (VNA). XRD confirmed the formation of magnetite after both the magnetic separation and milling processes. The results revealed that Fe3O4 exhibited excellent microwave absorption properties because of the synergistic characteristics of its dielectric and magnetic loss. The results showed that the Fe3O4/CM particle powder had a greater absorption power (reflection loss: <−10 dB) with 99.9% absorption, a minimum reflection loss of −30.83 dB, and an effective bandwidth of 2.30 GHz for 2 mm thick samples. The results revealed the Fe3O4/MM powders had higher absorption properties, including a higher RL of −20.59 dB and a broader bandwidth of 2.43 GHz at a matching thickness of only 1 mm. The higher microwave absorption performance was attributed to the better impedance matching property caused by the porous microstructure. Furthermore, the magnetite, Fe3O4 showed superior microwave absorption characteristics because of the lower value of permittivity, which resulted in better impedance matching. This study presents a low-cost approach method by reutilizing mill scale waste to fabricate a high purity crystalline Fe3O4 with the best potential for designing magnetic nano-sized based microwave absorbers.
11 October 2018 in Journal of Materials Science: Materials in Electronics
The parallel evolution of microstructure development via grain size changes from a nano-to-micron size regime toward multiferroic property development has been established in this research work. This kind of observation is not present in the literature in this research area, and studies of the link between morphological properties and ferroelectric properties of multiferroic materials have been focusing solely on the product of the ultimate sintering temperature, mostly neglecting the parallel evolutions of morphological properties and their relationship at varied chosen sintering temperatures. Holmium manganese oxide and yttrium manganese oxide were both prepared via high-energy ball milling (HEBM) in a hardened steel vial for 12 h. The pressed pellet went through multi-sample sintering, whereas the samples were sintered starting from 600 to 1250°C with 50°C increments for any one sample being subjected to only one sintering temperature. Orthorhombic HoMn2O5 and YMn2O5 phases were observed to exist in both as milled powder. The degree of crystallinity increased with increasing sintering temperature. Hexagonal HoMnO3 peaks were observed for sintering temperature ≥1050°C. As for YMnO3 series, the single phase of hexagonal YMnO3 started to appear at sintering temperature ≥1000°C. FESEM micrographs revealed that as the sintering temperature increased, the grain size increased, consequently increasing the geometric ferroelectric behavior. The polarization-electric field (P-E) plot reveals that HoMnO3 and YMnO3 are highly leaky ferroelectrics with a P-E curve shape different from the normal shape of highly insulating ferroelectrics. It shows that the remanent polarization and electric field increased generally with increasing grain size. For both series, there existed a difference based on their difference of crystallinity, microstructure data, and phase purity changes. Larger grain size is known to give ease for polarization to take place.