In this paper, two extraction methods for kenaf fiber, The chemical process and the enzymatic one, were performed. These processes were used to extract fibers from the kenaf stem and the chemical, mechanical and morphologic properties of the extracted fibers were investigated. We notice that the fiber diameter decrease when increasing the concentration of the enzyme and the time treatment (101,35 µm for Enz1 and 91,37 µm for Enz4) the same result is obtained for the chemical extraction when increasing the duration, temperature or NaOH concentration. Also the fiber crystallinity index is improved due to the elimination of the noncellulosic materials from the fiber. The results obtained show that we have an increase in this index for all treated fiber however it is more important for the chemical extraction (crude fiber 57.39%, chemical-treated fiber 71.93% and 66.70% for the enzyme-treated fiber). This increase explains also the increase of fiber tenacity and the decrease of strain and we found through the tensile test that kenaf fiber has a pure elastic behavior for all treated fiber. So, the properties of extracted fibers compared to the crude fibers prove that the enzymatic extraction preserves more the fiber structure than the chemical extraction.
The kenaf fibers were used to reinforce composites with two structures: nonwoven and bulk fibers and with treated and untreated kenaf fiber. A series of tensile tests were conducted on these composites. The use of kenaf fibers allows having composite with improved mechanical properties compared to pure polyester composite. This increase reaches 56.15% in strength and 137.85% in strain when varying the fiber weight ratio and the reinforcement structure. The interested results for both tensile strength and strain are obtained for nonwoven structure made by untreated fiber. The statistical study reveals that the most influencing parameter in tensile properties was the reinforcement weight ratio. The optimum composite was obtained when using a nonwoven structure made with untreated fiber with 11.10% fiber weight ratio.
This paper presents the results of the first kenaf spinning attempt in Tunisia. Indeed, kenaf fibers are rigid and lack of cohesion that makes their spinning difficult and a challenge. So, this paper describes the possibility of spinning different blends of kenaf/cotton fibers using open end spinning machine. Five different blends of kenaf/cotton (M1:10/90, M2:20/80, M3:30/70, M4:40/60, and M5:50/50) were considered. The higher kenaf content in the blend make spinning process difficult and even impossible. The produced yarns were characterized to evaluate their mechanical properties and compare it to similar yarn performances. These blends gave different yarn counts varying from 41.86 to 69.16 tex, tenacity of 8.80 cN/tex to 10.07 cN/tex, while elongation at break of 7% to 8.93%. The results proves that kenaf/cotton 40/60 blend ratio presents the better mechanical properties and regularity with 8.80 cN/tex for tenacity and 7.68% for elongation with good regularity index Ireg = 1.25.