Coal gangue, a major industrial solid waste from coal mining and processing, requires efficient alumina and silica separation for high-value utilization. This study focused on mineral reaction mechanisms and characteristics of coal gangue during calcination and alkaline leaching. Results showed calcination at 900–1200 °C altered its phase composition, affecting silica separation efficiency, with the optimal calcination range being 960–1120 °C. Poorly crystallized mullite and Al2O3 in calcined gangue were insoluble under low-alkaline and low-temperature conditions. On the contrary, amorphous silica is soluble and forms a sodium silicate solution in the proper alkaline conditions. This characteristic facilitates the efficient separation of alumina and silica. It was determined that the suitable conditions for silica removal from coal gangue are as follows: 1080 °C calcination for 90 min, leaching at 75 °C with 200 g/L NaOH (solid–liquid ratio of 1:4) for 4 h. Under these selected conditions, the silica leaching efficiency was 77.31%, the alumina leaching efficiency was 12.21%, the Na2O content in the leached residue was 1.94%, and the mass ratio of alumina to silica (A/S) in the leached residue increased from 0.88 to 3.42. A potential desilication mechanism was also analyzed.
In this study, the sintering behavior and electrical properties of 0.7Pb(Zr0.46Ti0.54)O3 (PZT)–0.1Pb(Zn1/3Nb2/3)O3 (PZN)–0.2Pb(Ni1/3Nb2/3)O3 (PNN) piezoelectric ceramics with different Pb(Fe2/3W1/3)O3 (PFW) doping contents were investigated to obtain a formulation that can be co-fired with silver (Ag) electrodes below 900 °C for multilayer ceramics. PFW was introduced as a sintering aid, which effectively reduced the sintering temperature of the ceramics from 1200 °C to 850 °C. The sample with x = 0.12 exhibited the largest average grain size of 1.72 μm, achieving excellent comprehensive properties with piezoelectric constant (d33) = 477 pC/N, planar electromechanical coupling factor (kp) = 0.68, dielectric loss tangent (tanδ) = 0.0154, and relative density of 98.2%. Furthermore, the feasibility of fabricating piezoelectric actuators based on this optimized composition was verified. Multilayer piezoelectric devices were prepared via screen printing combined with a carbon-based sacrificial layer method. No obvious interdiffusion was observed at the interface between the Ag internal electrodes and the ceramic matrix. The 9-layer device attained a high d33 = 1470 pC/N and produced a large displacement of 5.5 μm (corresponding to a strain = 1.83%) with a voltage of 500 V. The thickness of the multilayer piezoelectric film was approximately 0.3 mm. Through this, the feasibility of manufacturing a multilayered actuator with an Ag electrode was confirmed through the composition of 0.58PZT–0.1PZN–0.2PNN–0.12PFW.