ZnO semiconductor-based photocatalysts are mainly studied for the elimination of toxic textile dyes. Metal-doped ZnO displays better performance for this purpose. Herein, Al-doped ZnO (Al–ZnO) was prepared using the mechanochemical calcination method with varying aluminum concentrations for the degradation of the persistent methylene blue (MB) dye. Various characterization techniques, including XRD, FTIR, FESEM, TEM, UV-DRS, and XPS, revealed the improved properties of 3% Al–ZnO in degrading the MB dye. It exhibits 96.56% degradation of 25 mg/L MB dye under 60 min of natural sunlight irradiation with a catalyst dose of 0.5 g/L at a natural pH of 6.4. A smaller particle size, a lower band gap energy of 3.264 eV, and the presence of oxygen vacancies and defect states all facilitate photocatalytic degradation. Radical scavenger experiments using ascorbic acid (for •O2−), 2-propanol (for •OH), and diammonium oxalate (for h+) confirmed the crucial role of superoxide (•O2−) and hydroxyl (•OH) radicals in the degradation mechanism. The achievement of 82.80% MB degradation efficiency at the 4th cycle validates the notable stability and excellent reusability of Al–ZnO.
This research investigates the preparation of boron-doped tin dioxide (B-SnO2) nanoparticles via a simple sol–gel method at various B loadings. X-ray diffraction (XRD) showed that B preserved the SnO2 crystal structure while reducing the crystallite size from 5.05 to 3.14 nm. X-ray photoelectron spectroscopy (XPS) confirmed the presence of B in 3% B-SnO2. Field-emission scanning electron microscopy (FESEM) showed more rounded domains in 3% B-SnO2, and transmission electron microscopy (TEM) showed the average particle size decreasing from 12.61 nm for SnO2 to 10.61 nm. Ultraviolet–visible diffuse reflectance spectroscopy (UV-DRS) showed a decrease in the band gap from 3.60 eV (SnO2) to 3.24 eV (3% B-SnO2). Under ultraviolet-C (UV-C, 200–280 nm) irradiation, 3% B-SnO2 decolorized 94.80% of methylene blue (MB) in 90 min, compared with 76.00% for SnO2, 9.40% for photolysis, and 11.77% for dark adsorption. Because UV-C photons exceed the band gap of all samples, the improvement is more likely related to smaller crystallites and B-induced defects than to band-gap narrowing alone. Scavenger experiments implicated superoxide radicals (•O2−), hydroxyl radicals (•OH), and photogenerated holes (h+). Efficiency fell moderately to 81.25% after four cycles. Thus, 3 mol% B is an effective level for UV-C decolorization of MB by SnO2.