Zhihong Zhong

Prof. Dr. Zhihong Zhong


Research Focus & Metrics

Academic Career Length

12Years (2015-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 November 2018 in Rare Metals
Verified
Journal Article
Closed access
PDF file
XXXin Xian
Xin Xian
ZZZhihong Zhong
Zhihong Zhong
LLLi‐Jing Lin
Li‐Jing Lin
ZZZhi‐Xiong Zhu
Zhi‐Xiong Zhu
CCChang Chen
Chang Chen
YWYu‐Cheng Wu
Yu‐Cheng Wu

18 November 2019 in Metals and Materials International
Verified
Journal Article
Closed access
PDF file
LLLijing Lin
Lijing Lin
XXXin Xian
Xin Xian
ZZZhihong Zhong
Zhihong Zhong
YWYu–Cheng Wu
Yu–Cheng Wu
PLPeter K. Liaw
Peter K. Liaw

15 September 2021 in Advanced Composites and Hybrid Materials
Verified
Journal Article
Closed access
PDF file
LLLijing Lin
Lijing Lin
XXXin Xian
Xin Xian
ZZZhihong Zhong
Zhihong Zhong
KSKuijing Song
Kuijing Song
CWChengyong Wang
Chengyong Wang
PLPeter K. Liaw
Peter K. Liaw

19 June 2020 in Journal of Adhesion Science and Technology
Verified
Journal Article
Closed access
CWChunyan Wang
Chunyan Wang
XLXianfen Li
Xianfen Li
ZZZhihong Zhong
Zhihong Zhong
KSKuijing Song
Kuijing Song
GWGuoping Wang
Guoping Wang
YWYucheng Wu
Yucheng Wu
Tungsten/steel joints are desired for fusion reactors and militarily applications, as it could combine the unique properties of these two dissimilar metals. In view of the large differences of physical and chemical properties between W and steel, diffusion bonding is considered to be the proper technique for joining of W to steel. In this paper, diffusion bonding of W to low activation ferritic/martensitic steel at 1050 °C with 50 MPa for 20 min by spark plasma sintering (SPS) were investigated. The results showed that direct diffusion bonding of W to steel was feasible. However, the formation of ferrite and carbide at the W/steel interface lowered the joint strength. Effects of the insertion of ductile interlayers (Nb, Nb/Ni) on the joining interface microstructure and mechanical properties of W/steel joints were studied. The detailed microstructural characterization revealed that Nb could prevent the formation of ferrite and carbide at the W/steel interface. The Ni promoted the interfacial diffusion between Nb and steel. The shear strength and Vickers hardness of the joints were evaluated.

18 June 2015 in Metals and Materials International
Verified
Journal Article
Closed access
PDF file
YYY. Yuan
Y. Yuan
ZZZhihong Zhong
Zhihong Zhong
ZYZ. S. Yu
Z. S. Yu
HYH. F. Yin
H. F. Yin
YDY. Y. Dang
Y. Y. Dang
YGY. Gu
Y. Gu

5 April 2018 in Journal of Adhesion Science and Technology
Verified
Journal Article
Closed access
QWQun Wen
Qun Wen
ZZZhihong Zhong
Zhihong Zhong
AYAnkang Yang
Ankang Yang
ZWZhiquan Wang
Zhiquan Wang
HZHaibin Zhang
Haibin Zhang
In order to refine the grain size of TiSi2 silicide and reduce the formation of micro-defects in the joint, and thereby increasing the joint strength of SiC ceramic brazed with Si-24Ti (wt.%), a small amount of SiC particulates were added in the brazing alloy. The microstructure and mechanical strength of SiC joints was investigated by using field emission scanning electron microscopy, energy dispersive X-ray spectroscopy, X-ray diffraction spectrometer, and shear strength test. The results indicated that SiC particulates enhanced the nucleation and grain refinement of the TiSi2 and Si phase. The adding of appropriate content of SiC (<1 wt.%) could effectively refine the size of TiSi2 phase and increase the fraction of Si-TiSi2 eutectic zone. However, excess addition of 1.5 wt.% SiC caused the coarsening of TiSi2 phase due to the clustering of added fine SiC particulates. With the increasing of SiC particulate content, the shear strength of the joints increased at first and then decreased. The maximum shear strength of 106.3 MPa of SiC joint was obtained for the joint brazed with 1 wt.% SiC addition, which was ~19% higher than that of the joint brazed without SiC particulates.