Additive manufacturing has huge development potential in the aerospace field. The hot-end components of aeroengines work in harsh environments, facing high temperatures and a demand for long service life. In this paper, high-cycle fatigue (HCF) tests of Ti6Al4V alloy at 400 °C by selective laser melting (SLM) under different stress ratios (−1, 0.1, 0.3, 0.5, and 0.8) were carried out, and the fracture surfaces were observed. The results show that the defects existing on the surface or subsurface are prone to become the origin of fatigue cracks. There is a large dispersion of the high-cycle fatigue life of the samples, especially at a low stress ratio. With the increase in the stress ratio, the fatigue failure area on the fracture surface gradually decreases, and the fracture surface gradually presents a mixed pattern of tensile endurance fracture and fatigue failure. Considering the influence of creep damage due to mean stress, models were established, respectively, for the fatigue behavior and time-related rupture behavior to predict fatigue life and conduct an assessment. Then, the two models were combined and the composite models were proposed using the linear damage law. Finally, the single fatigue model and rupture models, as well as the composite models, were evaluated, respectively, and compared with the actual fatigue life, and the best model was obtained for the high-cycle fatigue prediction of SLM Ti6Al4V at 400 °C.
1 April 2026 in Journal of Physics: Conference Series
This study examines how selective laser-melted (SLM) GH3536 alloys behave under tension when tested in two different directions. The strength of the material changes significantly depending on the pulling direction. When the force is applied in the same direction as the build (BT), the strength is highest. When the force is applied along the laser scan direction, with the surface perpendicular to the sideways orientation (ST), the strength is lower but still moderate. This difference in strength is due to the way the material’s microstructure is formed during SLM: in the BT direction, the material has long, well-connected columnar grains and strong melt-pool connections, which make it stronger. In the ST direction, stress interacts with defects aligned with the laser scan paths, producing a mix of fracture types and resulting in lower strength.