The proliferation of single‐use plastics has stimulated interest in sustainable material substitutes with sufficient ductility and structural integrity. Herein, the mechanical behavior and high formability of the leaf sheath from a representative palm species—Areca catechu—and its immense potential for manufacturing of eco‐friendly food packaging are reported on. Using microstructural analyses, such as X‐ray micro‐computed tomography (μCT), electron microscopy, and optical profilometry, under different loading conditions, it is shown that this leaf can accommodate forming strains as large as 200%, similar to ductile metals. The sheath deformation response is highly sensitive to hydration, with up to 400% increase in forming strain. The embodied energy for leaf products is four to five orders smaller than for plastic or paper products. The results establish the microstructure basis for the high formability and the contours of a forming limit diagram that delineates product shapes that can be formed in a single step from this plant material.
1 December 2021 in Journal of The Royal Society Interface
Diffusion of water into plant materials is known to decrease their mechanical strength and stiffness but improve formability. Here, we characterize water diffusion through areca palm leaf-sheath—a model plant material, with hierarchical structure, used in eco-friendly foodware. The diffusion process is studied using mass gain measurements and in situ imaging of water transport. By treating the areca sheath as homogeneous ensemble, and incorporating effects of material swelling due to water absorption, a factor typically neglected in prior studies, the diffusion coefficient
D
w for water is estimated as (6.5 ± 2.2) × 10 −4 mm 2 s −1 . It is shown that neglecting the swelling results in gross underestimation of
D
w . Microstructural effects (e.g. fibre, matrix) on the diffusion are characterized using in situ imaging of the water transport at high resolution. The observations show that the water diffuses an order of magnitude faster in the matrix (8.63 × 10 −4 mm 2 s −1 ) than in the fibres (7.19 × 10 −5 mm 2 s −1 ). This non-uniformity is also reflected in the swelling-induced strain in the leaf, mapped by image correlation. Lastly, we vary salt concentration by controlled additions of NaCl and note a non-monotonic dependence of the diffusion on concentration. Implications of the results for improving foodware manufacturing processes and product life are discussed.