Fe-based metallo-supramolecular polymer (polyFe), composed of Fe(II) ions and bis(terpyridyl)benzene, is known as a good electrochromic (EC) material. For the first time, to improve the EC properties, we prepared nanocomposites comprising polyFe and a layered inorganic–imidazoline covalently bonded hybrid (LIIm) by simply mixing them in methanol and then examined the effect of the nanocomposition on EC properties. The obtained blue/purple-colored composites (polyFe/LIIm composites) were demonstrated by scanning electron microscopy (SEM) to comprise a structure of LIIm nanoparticles coated with amorphous polyFe. Interestingly, X-ray diffraction (XRD) measurements suggested that there was no intercalation of polyFe in the interlayer space of LIIm. Ultraviolet-visible (UV-vis) spectroscopy measurements demonstrated that light absorption close to 600 nm was attributed to metal-to-ligand charge transfer (MLCT) from the Fe(II) ion to the bisterpyridine ligand and was influenced by LIIm in the composites. The composites exhibited a pair of redox waves, assigned to the redox between Fe(II) and Fe(III), in the cyclic voltammograms; moreover, the composites were estimated to be diffusion controlled. Thin composite films demonstrated reversible EC changes, triggered by the redox reaction of the metal. Furthermore, the results show that the nano-scale composition of the metallo-supramolecular polymers with LIIm can effectively improve the memory properties without reducing the contrast in transmittance (ΔT) of 70–76% in EC changes after applying 1.2 V vs. Ag/Ag+. The EC properties varied with varying ratios (3/0.1, 0.5, 1, and 5) of the polyFe/LIIm, and the ratio of 3/1 exhibited the longest memory and largest MLCT absorption peak among composites. The results show that the polyFe/LIIm composites are useful EC materials for dimming glass applications, such as smart windows.
16 June 2016 in Physical Chemistry Chemical Physics
Through various in situ analyses, we have revealed the structural changes that occur during the reversible melting–solidification process of layered alkylsiloxanes (CnLSiloxanes) with carbon numbers (n) of 18 and 16. In situ high-resolution solid-state 13C nuclear magnetic resonance (NMR) analysis at controlled temperatures indicates drastic conformational changes of the long alkyl chains during the melting–solidification process. A 13C NMR signal at 33 ppm, which shows the highest intensity at room temperature (RT), is assigned to an inner methylene group with an all-trans conformation. As the temperature increases, the 33-ppm signal intensity decreases while the signal intensity at 30.5 ppm simultaneously increases. The 30.5 ppm signal is assigned to an inner methylene group with a trans–gauche conformation. Subsequently, upon cooling, the signal at 33 ppm recovers, even after CnLSiloxanes have melted. In situ X-ray diffraction measurements at controlled temperatures reveal that the ordered arrangement of the long alkyl chains becomes disordered with elevating temperatures and reordered upon cooling to RT. In situ high-resolution solid-state 29Si NMR analysis shows that the melting–solidification process progresses without any structural change in siloxane sheets of the CnLSiloxanes. Thus, the in situ analyses show that disordering of the long alkyl chains causes the CnLSiloxanes to melt. Because the majority of long alkyl chains are packed again in the ordered arrangement with the all-trans conformation upon cooling, the CnLSiloxanes are reversibly solidified and the CnLSiloxane structure is recovered.
6 February 2022 in Journal of Materials Chemistry C
The ambipolar triclinic C60/Fc nanosheet FETs were converted to n-type face-centered cubic C60 nanosheet FETs due to the loss of ferrocene with void formation upon heating at 150 °C.
Li+ ion-conducting glasses were prepared in the system Li2O–TiO2–P2O5 by rapid quenching. These glasses had high ionic conductivities of 10−2–10−5 S m−1 at 400 K. The conductivities of these glasses increased and the activation energy for conduction decreased with an increase in the Li2O content of the glasses. At a given Li2O content, the conductivities at 400 K increased with substituting TiO2 for P2O5.