Different profile structures were designed for a high-power engine piston, and engine tests were carried out to analyze and compare the influences of the widest point position and contraction rate on the skirt wear property. The results show that the lower position of the widest point will cause poor guidance, and at the same time the rapid radial reduction in both the upper and lower parts will increase the swing angles and the kinetic energy; the uniformity of wear loads can be improved effectively by increasing the height of the widest point and the width of the maximum diameter region; the degree of wear of the skirt can be considered through a comparison of the outer diameter variation.
Because of the microstructural anisotropy for laser cladding materials, the tribo-corrosion performance can vary significantly with different directions. In this study, one certain Fe-based coating was fabricated by laser cladding. To study the effects of anisotropy, three working surfaces (0°, 45°, and 90° to the building direction) were machined from the laser cladding samples; as-cast samples with an approximately homogeneous structure were prepared as controls. The tribo-corrosion tests were conducted in a 3.5 wt% NaCl solution with varying normal loads (5, 10, and 15 N). The results demonstrated that the 45° surface has superior friction stability, corrosion resistance, and wear resistance. This was directly related to the crystal orientation and grain boundary density. In addition, a refined microstructure may enhance tribo-corrosion properties by increasing deformation resistance and decreasing surface activity.
Different γ-Ni/Mo2Ni3Si alloy coatings were fabricated on 0.45 wt-% C steel applying the DISTA300 semiconductor laser system. The microstructures, phase components and corrosion behaviour of the alloy coatings were investigated. Research results showed that laser-cladded coatings with different compositions were all composed of ductile phase γ-Ni and reinforced phase Mo2Ni3Si. Electrochemical parameters and anodic polarisation curves revealed that the γ-Ni/Mo2Ni3Si alloy coatings exhibited a good corrosion performance in 3.5% NaCl solution in comparison with 0Cr18Ni9Ti stainless steel. The corrosion current density of the laser-cladded layer increased first and then decreased with the increasing volume fraction of Mo2Ni3Si. Moreover, the addition of Cr can significantly improve the passivation and anti-pitting ability of the γ-Ni/Mo2Ni3Si alloy coating.
19 November 2024 in Journal of Thermal Spray Technology
A series of γ-Niss/Mo2Ni3Si composite coatings were deposited on the hot-rolled 0.45 wt-% C steel plate using DJ-HL-T5000B CO2 laser system. The microstructure and phase constitution were studied by XRD and SEM with an attached EDS. Microhardness, toughness and dry sliding wear behaviour of the alloy coating were studied. Research results show that all the designed coatings with different compositions are composed of γ-Niss and Mo2Ni3Si. The volume fraction of Mo2Ni3Si, as well as the average microhardness, shows an increased tendency as the Ni content decreases from 65% to 50%. The addition of γ-Niss ductile phase can effectively improve the toughness of Mo2Ni3Si-based alloy and prevent the spread of the cracks. Furthermore, the wear resistance of laser-cladded γ-Niss/Mo2Ni3Si coatings exhibits a distinct improvement compared with that of the substrate. The wear mass loss and wear mechanism are affected by the volume fraction of Mo2Ni3Si.
Mg alloys are highly attractive for biodegradable surgical clips because of their low density and good biocompatibility; however, their limited strength and ductility restrict their widespread application. To overcome this limitation, this study employed screw rolling (SR) to produce a Mg–3Zn–0.2Ca alloy with a fine microstructure and an average grain size of 1.6 µm. Experimental results showed that the SR process improved the comprehensive tensile properties of the alloy, increasing the yield strength, ultimate tensile strength, and elongation from 192.6, 234.4 MPa, and 21.7% for the pre-extruded alloy to 252.3, 289 MPa, and 39.5%, respectively. Quantitative analysis of the strengthening behaviour identified grain refinement as the primary strengthening mechanism, along with considerable contributions from Orowan and dislocation strengthening. The ultra-high-tensile ductility was primarily attributed to the low internal stress, nano-sized precipitates, texture weakening, and activation of multiple slip systems. These findings provide a strategy for simultaneously increasing the ductility and strength of Mg alloys and lay a foundation for applying them as biodegradable clips.