One of the most critical components of super critical water reactor (SCWR) plant is pipe bend, carrying massive volume of supercritical water. Because of its intense fluctuation of velocity and pressure, it can exhibit unusual flow pattern in pipe bends conveying fluid. This unusual flow pattern may destroy the integrity of the piping network. Alternatively, because of unique chemical and physical properties, transportation of SCW can adversely effect on the integrity of the pipe bends, indicating probable failure of piping network. Therefore, intensive studies of SCW flow in bends are a must as a part of designing an efficient plant piping network. This article presents CFD analysis, carried out to examine the effect of variable pipe bend angle (90 deg, 120 deg, and 135 deg) on turbulent flow of SCW. The analysis indicates that the portion of the straight inlet pipe with fully developed flow shows no variation of results in all bend configurations. The study also reveals that secondary currents strengthen at lower bend angles and culminate the formation of vertices at the outlet of the right-angled elbow. It is found from the study that a greater part of the cross-sectional area is covered by the vortices at the bend midplanes compared to the bend outlets, where mixing of stream wise flow occurs as well. It is revealed that the radial positions of each vortex center are closer to the circumference of the pipe, and appear to be insensitive to bend angle. The study is ended with the comparison between supercritical water and normal water at standard conditions.
31 December 2020 in Progress in Solar Energy and Engineering Systems
This paper represents the characterization process of mono-facial solar cell in Bangladesh Atomic Energy Commission (BAEC) Lab. Mono-facial solar cell characterization performance analysis using surface reflection method, Sheet resistance method, SEM, Surface photo voltage and LIV test. The morphology of silicon wafer surface has been studied using scanning electron microscopy. It is found that the pyramid type structures are formed on the textured surface which helps to trap more light during conversion to electricity. The sheet resistance of raw and diffused sample is measured by using four point probe method. Results show that the resistivity of the wafer is decreased after diffusion which indicates the formation of n-type layer during diffusion process. The surface photo voltage data is used to find the diffusion length and life time. It is found the diffusion length 81.5μm and life time is 2.5μs. Finally, the efficiency of monofacial solar cell measured by LIV tester. Results show that the monofacial solar cell achieved fill factor (FF) of 0.310423 with a conversion efficiency (η) of 5.193843% where the active surface area is 96 cm2.