This paper examines the use of sheep wool and recycled aggregates (recycled concrete aggregate, reclaimed asphalt aggregate, recycled brick aggregate) in mortars. Nine cement mortars were prepared: a reference mortar with natural aggregate and no fibers, and eight mortars with 30% recycled aggregate, either fiber-free or micro-reinforced with 0.1% by mass of sheep wool fibers. The study investigates the effects of these components on the workability, mechanical properties, and microstructure of mortars. Micro-reinforcing mortars with sheep wool fibers or partially replacing natural aggregate with recycled aggregates reduces workability by up to 32%. Mortars with recycled concrete and recycled brick aggregates showed increased compressive and flexural strength compared to the reference mortar. The combined formulation (recycled brick with sheep wool micro-reinforcement) achieved the highest compressive strength, increasing by 24.3% while maintaining excellent flexural performance. Three-point bending tests with displacement control revealed improved post-crack behavior and greater ductility in fiber micro-reinforced specimens compared to those without fibers. The results support the use of sheep wool fibers in mortars, demonstrate the satisfactory performance of recycled aggregates, and indicate promising potential for formulations combining sheep wool fiber and recycled aggregate as sustainable and waste-reducing alternatives in mortars.
This study investigates the effects of agro-waste-based capsules made from grape seeds and cherry pits on the physical, mechanical, thermal and self-healing properties of concrete. Capsule-containing mixtures were compared with a reference concrete after 28 days of water curing using both standardized and non-standardized testing methods. Capsule incorporation reduced workability by up to 91% and altered air content depending on capsule type, increasing it by 47% for grape seed capsules and decreasing it by 65% for cherry pit capsules. Fresh concrete density was reduced by 5.5% and 6.8% for grape seed and cherry pit capsules, respectively, while hardened concrete density decreased by 11% and 9%, implying lighter structures with improved seismic resistance. Compressive strength decreased by 49% for grape seed capsules and 27% for cherry pit capsules. Thermal conductivity was reduced by 32% and 22%, respectively, indicating improved energy efficiency. Concrete with grape seed capsules showed freeze–thaw performance comparable to the reference concrete after 112 cycles, whereas concrete with cherry pit capsules exhibited superior dynamic modulus behavior, suggesting continuous crack healing, despite significant mass loss due to poor capsule–matrix bonding. SEM analysis showed no significant crack reduction, while EDS revealed calcium-rich areas in grape seed capsule concrete, indicating possible crack healing. Overall, agro-waste capsule concrete shows potential for improving seismic resistance and energy efficiency, although further research is required to clarify the self-healing effect.
This study investigates the fire resistance of alkali-activated mortar incorporating crushed brick as both a precursor and aggregate. The optimal alkaline activator was identified as a combination of KOH and Na₂SiO₃, with a curing period of 3 days at 70 °C. Two mortar series were produced, each exhibiting different workability: on series comprised cement mortar, while the other included three alkali-activated mortars, with variations in the molarity of the KOH solution. The mortar samples were subsequently heated to 600°C, and their mechanical properties and mass were measured to determine residual values/losses. The best-performing alkali-activated and cement mortars underwent visual assessments of cross-sections to evaluate the impact of mortar consistency on fire resistance. Additionally, changes in mineralogy and microstructure were followed by instrumental techniques to clarify the results before and after heating. While cement mortars had superior mechanical properties at room temperature, alkali-activated mortars retained a higher percentage of their mechanical properties post-heating, demonstrating better fire resistance. Mortars with plastic consistency showed better fire resistance than those with fluid consistency. These findings suggest that brick-based alkali-activated mortars could be developed into fire protection boards for structural members. Doi: 10.28991/CEJ-2025-011-04-05 Full Text: PDF
Technobius is a peer-reviewed open-access journal that publishes original research articles of experimental and technical nature in the field of construction and building materials
In this study, brick plant waste was used to produce alkali-activated mortars. Four mixtures with identical compositions but different mixing sequences and curing methods were prepared. Two were conventionally produced using a pre-cooled 10 M potassium hydroxide (KOH) solution and sodium silicate (Na2SiO3), with one cured at ambient conditions and the other at an elevated temperature. The remaining two used modified mixing sequences to utilize internally generated heat for curing (direct KOH powder addition and addition of KOH dissolved in water immediately before mixing). The influence of mixing sequence and curing method on mechanical properties and high-temperature performance was evaluated after exposure to 600 °C through residual flexural and compressive strengths, mass loss, and visual examination of specimen cross-sections. The two best-performing mortars were further characterized by Fourier-transform infrared spectroscopy (FT-IR) and field-emission scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (FE-SEM-EDS), while the mixture combining favorable high-temperature performance with simple preparation was additionally analyzed for thermal conductivity and specific heat capacity. The conventionally prepared, elevated-temperature-cured mixture exhibited the lowest room-temperature flexural and compressive strengths (2.7 and 12.9 MPa, respectively) but the best high-temperature performance, with flexural and compressive strength increases of 14.8% and 10.9%, respectively, after exposure to high temperature. Visual assessment may suggest some degree of structural densification in this mixture and in the mixture prepared by direct addition of KOH powder to the dry components, whereas the other two mixtures may exhibit signs of partial weakening in the interfacial transition zone (ITZ). Among the internally cured mixtures, direct KOH powder addition produced slightly better room- and high-temperature performance than adding KOH dissolved in water immediately before mixing. FT-IR and FE-SEM-EDS confirmed the formation of potassium and sodium aluminosilicate hydrate, (K,N)-A-S-H, gel in the conventionally prepared, elevated-temperature-cured mixture and the mixture with direct KOH powder addition. The nearly unchanged compressive strength of the KOH-powder-based mixture was associated with a high retention of thermal conductivity (93%) and specific heat capacity (80%) after high-temperature exposure.
The construction sector relies heavily on virgin mineral resources and produces significant quantities of construction and demolition waste. This study examines crushed brick aggregate (CBA) as a volumetric substitute for natural river sand in micro-concrete at replacement levels of 0%, 25%, 50%, 75%, and 100%. Results show that increasing CBA content decreases consistency and flexural strength while increasing water absorption. However, compressive strength is maintained even at full replacement. One-way ANOVA demonstrated significant overall effects of CBA replacement level on all investigated properties. However, Tukey’s HSD comparisons indicated that not all adjacent replacement levels exhibited significant differences. Specifically, compressive strength at 25% and 50% replacement did not differ significantly from the reference mixture. A nominal resource-efficiency assessment based on the absolute-volume method and literature-derived density values indicates that, at 25% volumetric replacement, the mixture incorporates approximately 286.7 kg/m3 of CBA and saves 362.4 kg/m3 of natural sand while retaining 94.3% of the reference compressive strength. For Croatia’s estimated 8882 t of waste bricks in 2024, a maximum yield scenario suggests production of about 30,985 m3 of this mixture and natural sand savings of approximately 11,231 t. The 25% replacement level offers the most balanced outcome in terms of secondary resource utilisation, consistency, mechanical performance, and water absorption.