The development of high-performance aqueous energy storage systems requires materials and strategies capable of simultaneously enhancing energy density while preserving high-power capability and long-term stability. In this work, we investigate the hydrothermal synthesis and provide a comprehensive theoretical-experimental study of the physicochemical properties of the metastable tetragonal bismuth oxide phase (β-Bi₂O₃). We also report the assembly and evaluation of a hybrid aqueous supercapacitor based on a β-Bi₂O₃ conversion-type negative electrode coupled with a reduced graphene oxide (rGO) positive electrode, utilizing a redox-mediated electrolyte containing the [Fe(CN)6]3⁻/4⁻ couple. The hydrothermally synthesized β-Bi₂O₃ exhibits a hierarchical structure composed of sub-micrometric aggregates of primary nanoparticles, enabling efficient charge storage through a six-electron conversion mechanism. First-principles calculations demonstrate that β-Bi₂O₃ combines a mechanically compliant framework, a narrow HSE06 band gap of 2.39 eV, low neutral oxygen-vacancy formation energies, and a reduced oxygen-migration barrier of 0.82 eV. These features support a labile oxygen sublattice suitable for oxygen-related rearrangements during conversion-type charge storage. In a three-electrode configuration, the β-Bi₂O₃ electrode delivers a high specific capacity of 304.9 mAh g⁻¹ at 1 A g⁻¹ with excellent rate capability. In the full-cell study, the introduction of the redox-active electrolyte effectively compensates for the intrinsic capacity mismatch between the β-Bi₂O₃ and rGO electrodes, significantly enhancing the charge storage performance of the positive electrode. The resulting hybrid device operates stably up to 2.0 V in an aqueous medium, enabled by the high hydrogen evolution overpotential of β-Bi₂O₃ and the kinetically limited oxygen evolution at the positive interface. The full cell delivers an energy density of 32.4 Wh kg⁻¹ at 1547 W kg⁻¹ and maintains 71% capacity retention after 5000 cycles.
A hybrid material based on the copolymerization of EDOT (3,4-ethylenedioxythiophene) and Py (pyrrole), 1:1 monomer ratio, onto multi-walled carbon nanotubes (MWCNTs) was synthesized through a multistep functionalization approach. The resulting P(EDOT-co-Py)@MWCNT hybrid, poly(3,4-ethylenedioxythiophene-co-pyrrol)@MWCNT hybrid, was characterized by Fourier-transform infrared spectroscopy (FTIR), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and thermogravimetric analysis (TGA). These characterizations confirmed the successive functionalization steps, the effective anchoring of the monomers, and the subsequent formation of the copolymer. Transmission electron microscopy (TEM) images revealed a homogeneous polymer coating along the nanotube surface, while preserving the structural integrity of the MWCNTs throughout the functionalization and polymerization processes. The P(EDOT-co-Py)@MWCNT hybrid was evaluated as an active electrode material for aluminum-ion storage in aqueous aluminum sulfate electrolyte. The system exhibited two distinct charge-storage mechanisms: at high current densities, proton surface adsorption dominated, whereas at lower rates, a faradaic contribution associated with polymer chain redox activity and the reversible extraction/insertion of Al³⁺ became prevalent. The hybrid electrode delivered high specific capacities, reaching 200.6, 106.3, and 44.3 mAh g⁻¹ at 0.10, 0.25, and 0.50 A g⁻¹, respectively. These values are comparable to—or even exceed—those reported for similar cathodic materials designed for Al³⁺ storage, highlighting P(EDOT-co-Py)@MWCNT hybrid as a highly promising cathode candidate for aqueous aluminum-ion energy-storage systems.
A hybrid material based on the copolymerization of EDOT (3,4-ethylenedioxythiophene) and Py (pyrrole), 1:1 monomer ratio, onto multi-walled carbon nanotubes (MWCNTs) was synthesized through a multistep functionalization approach. The resulting P(EDOT-co-Py)@MWCNT hybrid, poly(3,4-ethylenedioxythiophene-co-pyrrol)@MWCNT hybrid, was characterized by Fourier-transform infrared spectroscopy (FTIR), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and thermogravimetric analysis (TGA). These characterizations confirmed the successive functionalization steps, the effective anchoring of the monomers, and the subsequent formation of the copolymer. Transmission electron microscopy (TEM) images revealed a homogeneous polymer coating along the nanotube surface while preserving the structural integrity of the MWCNTs throughout the functionalization and polymerization processes. The P(EDOT-co-Py)@MWCNT hybrid was evaluated as an active electrode material for aluminum-ion storage in an aqueous aluminum sulfate electrolyte. The system exhibited two distinct charge-storage mechanisms: at high current densities, proton surface adsorption dominated, whereas at lower rates, a faradaic contribution associated with polymer chain redox activity and the reversible extraction/insertion of Al3+ became prevalent. The hybrid electrode delivered high specific capacities, reaching 200.6, 106.3, and 44.3 mAh g−1 at 0.10, 0.25, and 0.50 A g−1, respectively. These values are comparable to—or even exceed—those reported for similar cathodic materials designed for Al3+ storage, highlighting P(EDOT-co-Py)@MWCNT hybrid as a highly promising cathode candidate for aqueous aluminum-ion energy-storage systems.