Cellulose triacetate (CTA) nanofibers were formed by electrospinning using two binary solvent systems: methylene chloride/ethanol and chloroform/acetone. Previously, licorice root cellulose (LRC) with a degree of polymerization (DP) of 710 was extracted from licorice root waste by alkaline treatment and hydrogen peroxide bleaching at high temperatures. Then CTA with a degree of substitution (DS) of 2.9 and an average molecular weight of 175 kDa was synthesized from LRC using acetic acid and acetic anhydride, sulfuric acid was as a catalyst. The influence of the electrospinning process and various solvent systems on the morphology and structure of nanofibers is studied. The structure and morphology of the nanofibers were characterized by Fourier transform infrared (FTIR) spectroscopy, X-ray diffraction, scanning electron microscopy (SEM), thermal gravimetric analysis (TGA), and the sorption characteristics were also investigated. The results showed that the morphology and structure of nanofibers depended on the solvent mixture used. The average diameters of the CTA nanofibers with grooved morphology varied 200-700 nm (solvent methylene chloride/ethanol) and the dumbbell-shaped (flat ribbon) CTA nanofibers in a wide range from 200 nm to 4 mkm (solvent chloroform/acetone).
Two-dimensional MXenes have emerged as a versatile class of materials for energy storage, electronics, and catalysis owing to their high electrical conductivity, tunable surface chemistry, and layered structure; however, the controlled synthesis of Ti3C2Tx MXene with well-defined morphology and stable surface chemistry remains a major challenge, as etching conditions strongly influence structural integrity, degree of exfoliation, and functional performance. In this study, the morphological, structural, and functional evolution of Ti3C2Tx MXene materials was systematically investigated by applying hydrofluoric acid (HF) etching at varying concentrations (6 %, 12 %, 24 %, 36 %, and 48 %) using microwave-assisted method. The impact of etching intensity on Al removal, layer delamination, and surface functionalization was examined through a multi-technique characterization approach including scanning electron microscopy (SEM), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), and energy-dispersive X-ray spectroscopy (EDS). The results reveal that an HF concentration of 24 % achieves efficient Al extraction while preserving the Ti–C framework, yielding well-exfoliated and structurally stable MXene sheets. Lower HF concentrations (6 % and 12 %) lead to incomplete etching and limited exfoliation, whereas higher concentrations (36 % and 48 %) cause over-etching and pronounced structural degradation. These findings underscore the critical role of etching conditions in tuning MXene morphology and functional properties. The ability to balance surface termination control and structural integrity via gradient etching is particularly relevant for the use of Ti3C2Tx MXenes as conductive electrodes and interfacial layers in photovoltaic and other energy-conversion devices.