This study present a series of finite element models for high-pressure jet-assisted machining of Ti-6Al-4 V alloy. The application of Fluid-Structure Interaction (FSI) together with the Johnson-Cook plasticity model, Cockcroft-Latham chip separation criteria and EOS polynomial were implemented to study the effect of coolant pressure on chip formation, cutting force and cutting temperature. The resulting motion of fluid at the tool-chip interface, chip breakage, cutting force as well as temperature generation at the tool-chip interfaceis then interpreted, analyzed and compared to their real experimental results. The models simulate interactions between the fluid and solid structure, where continuous chip formation was observed when simulation in conventional coolant supply while chip breakage was clearly evident as high-pressure coolant was introduced. Increasing coolant pressure significantly reduce the friction at the tool-chip interface, which significantly reduced the cutting force and cutting temperature.
The sintering temperature and holding time have a significant impact on the densification of a ceramic compact. In this study, alumina inserts were made with varying sintering temperatures and holding times. The procedure began with the compacting of alumina powders inside a mould with trapezium and round shapes. These inserts were then sintered between 1200 °C and 1400 °C for 5 to 9 h holding time. The sintered samples underwent analysis based on the shrinkage size, density, and microstructure. The sample with the highest density was chosen for additional machining tests. The results showed that the alumina shrinkage ranged from 3 to 6%, with a maximum relative density of 91.3% recorded when the sintering parameter was applied at 1400 °C and a 9 h holding time. The transition of the grain growth was observed depending on the sintering temperature and heating duration. When machined with AISI 1045 carbon steel, the sintered alumina inserts achieved a maximum tool life of 35 s at a cutting speed of 350 m/min. The sintered inserts exhibited brittle characteristics with a dominant notch wear and abrasive mechanisms.
This study focuses on the fabrication of alumina based cutting tool for machining application. Specific weight of alumina powders were pressed in a mold using hydraulic press at 8 tons before compressed through Cold Isostatic Press (CIP) at 30000 psi. Green body then was dried and sintered at 1700 °C at 4 hours sintering time to form solid cutting tools. These cutting tools were then tested in turning operation to machine AISI 1045 with different cutting speeds. The results shows that CIP pressed alumina cutting tool obtained the hardness of 83.2 HRA which is considered adequate to machine AISI 1045 steel. The shrinkage of alumina powders recorded about 7% form green compact to sintered body. In terms of flank wear, the alumina cutting tool demonstrated decreased wear rate as the cutting speed increased from 150 m/min to 225 m/min. Wear area focused at the edge of cutting tool due to small nose radius with the minimum wear rate recorded at 0.0025 mm/s for 225 m/min cutting speed. The newly fabricated cutting tools can be improved if finer or secondary reinforced particles were used.
Cutting tools can be considered major industrial necessities as it applied mostly in parts production. Development of self-fabricated cutting tool can facilitate lower machining cost as long as the cutting tool can perform effectively. This paper presents the fabrication of the alumina based ceramic cutting tool where the study begins from the mould development until machining tests. Ceramic cutting tools are developed through solid-state methods consisting of pure alumina, zirconia toughened alumina (ZTA) and Zirconia toughened alumina doped Cr2O3 (ZTA doped Cr2O3). To assess the performance and lifetime of the cutting tool, CNC turning machines are used for this tests while optical microscopes for wear measurements and Scanning Electron Microscopy (SEM) are used to analyse the wear mechanism. The aim of this study is to develop ceramic cutting tool and performances comparison on AISI. Solid-state method is used with processing carried out through a ceramic powder mix using ball mill machine for 12 hours and 40 rpm, then the green body is formed by mechanical pressing and CIP to make a high compaction of the green body at 300 MPa pressure. The 1400oC sintering process is enough to obtain a powerful cutting tool to obtaining the highest hardness of HV 13 GPa and HRC 71.3 on ZTA doped by Cr2O3. CNC lathe machining with cutting speed 150 m/min, 200 m/min, 250 m/min, 300 m/min and 350 m/min, feed rate of 0.125 mm/rev per cutting speed and 0.5 mm depth of cut is used. The results show that ZTA doped Cr2O3 has the highest life span of 360 seconds and it shows that the Cr2O3 addition can improve machining reliability.
1 February 2021 in Journal of Physics: Conference Series
This study presented the effect of pressure on the density, porosity and flexural strength when cold isostatic press (CIP) was applied to compact the ceramic powders in the form of insert cutting tools. Specific composition of alumina (Al2O3) wt.90%, yittria stabilized zirconia (YSZ) wt.10%, chromium oxide(Cr2O3) wt.0.6% and polyethylene glycol (PEG) wt.0.6% were ball milled and hand pressed to form green body of ceramic inserts. These green body were undergone further compaction inside CIP with pressures variation of 200 MPa, 300 MPa, 400 MPa with 30 seconds and 60 seconds pressuring time. The ceramic composts were then sintered at 1440°C for 9 hours before being assessed with density, porosity, Rockwell hardness (HRC) and bending test. The results show that CIP use with 300 MPa parameters with 60 seconds shows the best mechanical properties with relative density 95.5%, porosity 4.5% and HRC 65.5 hardness. Further assessment of microstructure revealed that the particles size distributed evenly along fracture surface with coarse grain and porosity dominant in the certain area.
The research regarding additive manufacturing methods (AM) is popular among new researchers from industrial workers or university students since this technology is most likely to pioneer manufacturing industries in the future. Almost all the studies conducted by past researchers are related to the material properties of the 3D printing machine regardless of the type of material including Selective Laser Melting (SLM) 3D printing machines which utilize metal powder as the primary material. Plus, there is a study on the difference between virgin and recycled powder material in terms of material properties for SLM 3D printing machines. In this study, we conducted Charpy impact tests on metal specimens fabricated from both virgin and recycled powders, varying the print thicknesses in accordance with ASTM E23 standards. For each thickness parameter, three specimens were produced, irrespective of the material state. The selective laser melting (SLM) machine maintained consistent printing parameters for both virgin and recycled materials, while permitting flexibility in the adjustment of specimen coordinates within the production bed. Therefore, the impact test result will determine which material condition delivers the best result of the specimens’ absorbed energy (J) and impact toughness (J/cm²).