In this study, we present the fabrication of nitrile butadiene rubber/waste leather fiber (NBR/WLF) composites with different weight percentages of WLF and NBR (0/100, 20/80, 30/70, 40/60, 50/50, 60/40 wt/wt). WLF was prepared by cutting the scrap leathers from the waste product of the Vietnamese leather industry. Subsequently, in order to make the short fibers, it was mixed by a hammer mill. The characteristics of WLF/NBR composites such as mechanical properties (tensile strength, tear strength, hardness), dynamic mechanical properties, toluene absorption, and morphology were carefully evaluated. As a result, the tensile strength and tear strength become larger with increasing WLF content from 0 to 50 wt% and they decrease when further increasing WLF content. The highest tensile strength of 12.5 MPa and tear strength of 72.47 N/mm were achieved with the WLF/NBR ratio of 50/50 wt%. Both hardness and resistance of the developed materials with toluene increased with increasing WLF content. The SEM results showed a good adhesion of NBR matrix and the WLF. The increasing of storage modulus (E’) in comparison with raw NBR showed good compatibility between WLF and NBR matrix. This research showed that the recycled material from waste leather and NBR was successfully prepared and has great potential for manufacturing products such as floor covering courts and playgrounds, etc.
Graphene has been demonstrated to be one of the most promising candidates to use as filler to improve the electrical, thermal, chemical and mechanical properties of natural rubber due to exceptional high surface area, superior electrical and thermal conductivity, and remarkable gas impermeability resistance. In this study, graphene nanoplates (GNPs) were mass-produced by a one-step chemical exfoliation of natural graphite and used as a filler for the fabrication of GNPs@natural rubber composite by a simple mixing method. The resultant GNPs/rubber composite was characterized by using scanning electron microscopy (SEM), and a rheometer. The prepared graphene nanoplates had a thickness of less than 10 nm and a lateral size of tens of microns. The GNPs@rubber composite revealed an exceptional improvement of abrasion loss up to seven to ten fold, along with an approximately 400%, 200% and 30% increment of elongation at break, tear strength and tensile strength, respectively. Other mechanical properties, such as hardness, compression set and rebound, as well as the effect of the GNPs loadings on the mechanical properties of the composite, were also investigated in detail.
This study aimed to improve the mechanical properties of a composite material consisting of waste leather fibers (LF) and nitrile rubber (NBR) by partially replacing LF with waste polyamide fibers (PA). A ternary recycled composite NBR/LF/PA was produced by a simple mixing method and vulcanized by compression molding. The mechanical properties and dynamic mechanical properties of the composite were investigated in detail. The results showed that the mechanical properties of NBR/LF/PA increased with an increase in the PA ratio. The highest tensile strength value of NBR/LF/PA was found to have increased about 1.26 times, that is from 12.9 MPa of LF50 to 16.3 MPa of LF25PA25. Additionally, the ternary composite demonstrated high hysteresis loss, which was confirmed by dynamic mechanical analysis (DMA). The presence of PA formed a non-woven network that significantly enhanced the abrasion resistance of the composite compared to NBR/LF. The failure mechanism was also analyzed through the observation of the failure surface using scanning electron microscopy (SEM). These findings suggest that the utilization of both waste fiber products together is a sustainable approach to reducing fibrous waste while improving the qualities of recycled rubber composites.
Mechanical responses after the uniaxial deformation of graded styrene–butadiene rubber (SBR) with a gradient in the crosslink points in the thickness direction were investigated as compared with those of homogenously vulcanized SBR samples. The elongational residual strain of a graded sample was found to depend on the part with a high crosslink density. Therefore, it showed good rubber elasticity. After stress removal, moreover, the graded sample showed a marked warpage. This suggested that shrinking stress acted on the surface with a high crosslink density, which would avoid a crack growth on the surface. The sample shape was then recovered to be flat very slowly, indicating that the shrinking stress worked for a long time. This unique rubber elasticity, i.e., slow strain recovery with an excellent strain recovery, makes graded rubber highly significant.
The rheological properties of a polyamide (PA) resin with low crystallinity were modified by melt-mixing it with a small amount of an alternative α-olefin–maleic anhydride copolymer as a reactive compound. Because PA has a low melting point, rheological characterization was performed over a wide temperature range. Owing to the reaction between PA and the alternative α-olefin–maleic anhydride copolymer, the blend sample behaved as a long-chain branched polymer in the molten state. The thermo-rheological complexity was obvious owing to large flow activation energy values in the low modulus region, i.e., the rheological time–temperature superposition principle was not applicable. The primary normal stress difference under steady shear was greatly increased in the wide shear rate range, leading to a large swell ratio at the capillary extrusion. Furthermore, strain hardening in the transient elongational viscosity, which is responsible for favorable processability, was clear. Because this is a simple modification method, it will be widely employed to modify the rheological properties of various polyamide resins.
18 October 2023 in Polymers for Advanced Technologies