Using samples of Co100−xTbx/Cu/Y3Fe5O12, we investigate the heat-to-charge current conversion phenomena in amorphous Co100−xTbx alloys. We find an enhancement of the inverse spin Hall voltage owing to the Tb impurity by means of the spin Seebeck effect. The spin Hall angle of Co68Tb32 is 3.5 times larger than that of Co, and mainly originates from the extrinsic spin Hall effect. Meanwhile, we detect an anomalous Nernst voltage owing to the magnetic properties of Co100−xTbx alloy. The sign of the inverse spin Hall voltage is observed to be the same for all Co100−xTbx samples, whereas the anomalous Nernst voltage changes its sign around the magnetization compensation composition. Our finding proves Co100−xTbx is an efficient spin-to-charge current convertor, and it has advantages for manipulating not only the inverse spin Hall effect but also the anomalous Nernst effect by means of adjusting the Tb concentration.

1 April 2024 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
MOMiho Odagiri
Miho Odagiri
HIHiroto Imaeda
Hiroto Imaeda
AYAhmet Yagmur
Ahmet Yagmur
YKYuichiro Kurokawa
Yuichiro Kurokawa
SSSATOSHI SUMI
SATOSHI SUMI
KTKenji Tanabe
Kenji Tanabe
The anomalous Nernst effect (ANE) has garnered significant interest for practical applications, particularly in energy harvesting and heat flux sensing. For these applications, it is crucial for the module to operate without an external magnetic field, necessitating a combination of a large ANE and a substantial coercive force. However, most materials exhibiting a large ANE typically have a relatively small coercive force. In our research, we have explored the ANE in amorphous ferrimagnetic TbCo alloy films, noting that the coercive force peaks at the magnetization compensation point (MCP). We observed that transverse Seebeck coefficients are amplified with Tb doping, reaching more than 1.0 μV/K over a wide composition range near the MCP, which is three times greater than that of pure Co. Our findings indicate that this enhancement is primarily due to direct conversion, a product of the transverse thermoelectric component and electrical resistivity. TbCo films present several significant advantages for practical use: a large ANE, the capability to exhibit both positive and negative ANE, the flexibility to be deposited on any substrate due to their amorphous nature, a low thermal conductivity, and a large coercive force. These attributes make TbCo films a promising material for advancing ANE-based technologies.

5 June 2020 in Applied Physics Express
Verified
Journal Article
Closed access
PDF file
JTJunji Tominaga
Junji Tominaga
SSSATOSHI SUMI
SATOSHI SUMI
HAHiroyuki Awano
Hiroyuki Awano
Phase-change memory using a superlattice composed of GeTe and Sb2Te3 periodic structures has been attracting attention for increasing switching speed and reducing energy consumption. However, so-called "atomic intermixing through the interfaces" was a major challenge for realizing devices. The effect was analysed by molecular dynamics simulation (MD), transmission electron microscopy (TEM) and spin transport. We found that S atoms significantly decrease the free energy of formation in the Ferro phase of GeTe, and the superlattice fabricated using a GeTe target with 3at% of S greatly suppress the intermixing.

13 November 2023 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
MMMojtaba Mohammadi
Mojtaba Mohammadi
SSSATOSHI SUMI
SATOSHI SUMI
KTKenji Tanabe
Kenji Tanabe
HAHiroyuki Awano
Hiroyuki Awano
This study highlights the significant achievement of enhancing domain wall (DW) velocity through the laser-annealing (LA) process in GdxFe100−x films, with a specific focus on the Gd26Fe74 composition. By investigating the current-induced DW motion, it was observed that the LA process on the edges and middle of the nanowires resulted in a remarkable improvement in DW velocity from around 600 m/s for non-laser-annealed to 1800 m/s for laser-annealed conditions. Furthermore, we conducted additional experiments to explore the stability and dynamics of a system involving DWs in a single wire. The experimental results revealed a stable and uniform movement of the DWs, as evidenced by a velocity of approximately 1800 m/s, even after the application of 20 pulses with a short pulse width of 1 ns. The resulting stability of the DW motion across a wide range of applied currents demonstrates the practical significance of the LA in achieving high-performance racetrack memories. Our findings suggest that the LA process has a similar effect on both the middle and edge treatments of the wire. This indicates that structural defects on the wire's edges are not the main cause of the observed low velocity or curvy shape of DWs. One possible mechanism for this effect is the reduction of the Ku value through the LA process. This study establishes a ground-breaking advancement by showcasing the effectiveness of the LA in enhancing DW motion velocity in GdFe ferrimagnetic thin films, thereby opening avenues for future research and industrial applications in this field.

24 September 2018 in Crystals
Verified
Journal Article
Open access
PDF file
SISyougo Iemoto
Syougo Iemoto
SSSATOSHI SUMI
SATOSHI SUMI
PTPham Van Thach
Pham Van Thach
HAHiroyuki Awano
Hiroyuki Awano
MHMasamitsu Hayashi
Masamitsu Hayashi
Magnetic films with a heavy metal layer show strong interfacial interaction of spin-orbit. Spin-orbit interaction is one of the key technologies for spintronics. In this paper, we measured magneto-optical Kerr spectra of Pt/TbCo hetero-structure films on a thermally oxidized silicon substrate (0.3 mm); A: Pt (3 nm)/TbCo (6 nm)/Pt (3 nm), B: Si3N4 (10 nm)/TbCo (6 nm)/Pt (3 nm), and C: Pt (3 nm)/TbCo (6 nm)/Si3N4 (10 nm). Magneto-optical Kerr spectra of each sample were measured with a wavelength range of 300–700 nm, and were compared to the simulated spectra using the effective refractive index method. In the sample A, which has a symmetric structure, the simulated spectra are consistent with the measured ones. On the other hand, in the samples B and C, with an asymmetric structure, there are some differences between the simulated spectra and the measured ones in a lower photon energy region. This may be caused by interfacial effects of the spin-orbit interaction.

1 September 2022 in APL Materials
Verified
Journal Article
Open access
PDF file
SRS. Ranjbar
S. Ranjbar
SSSATOSHI SUMI
SATOSHI SUMI
KTKenji Tanabe
Kenji Tanabe
HAHiroyuki Awano
Hiroyuki Awano
Architectures based on multi-bit magnetic domain walls (DWs) take advantage of the fast speed, high density, nonvolatility, and flexible design of DWs to process and store data bits. However, controlling multi-bit DWs driven by electric current at an ideal position remains a significant challenge for developing integrated spintronic applications with high reliability and low power consumption. We exhibit the possibility of driving fast and stable multi-bit DWs at low current density without an in-plane external magnetic field in Fe-rich GdFeCo magnetic wires. When an in-plane magnetic field is applied in the wire direction, the front edge accelerates, although the rear edge decelerates, and the recorded data are destroyed. Hence, this method is not practical. Here, the DW speed of the multi-bit DWs is 1500 m/s under a low current density of 29 × 1010 (A/m2). A straight DW shape is required to accurately read the bits of information by the tunneling magnetoresistance head in real DW memory devices. Moreover, we demonstrate that the DW position is related to the DW shape after injecting a pulse current into the magnetic wire. A straight DW shape is exhibited for 3 ns pulse duration width, while the DW shape became rounded for 30 and 50 ns pulse duration widths. Our finding provides a practical concept for multiple-bit-per-cell memory and presents a viable platform for DW memory applications.