Guonan Ma

Dr. Guonan Ma

orcid

Research Focus & Metrics

Academic Career Length

2Years (2025-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 March 2026 in Coatings
Verified
Journal Article
Open access
PDF file
JZJinyu Zhu
Jinyu Zhu
YDYangping Dong
Yangping Dong
HZHuihua Zhang
Huihua Zhang
SZShuming Zhao
Shuming Zhao
GMGuonan Ma
Guonan Ma
PXPeng Xu
Peng Xu
A Ti6Al4V alloy fabrication via laser powder bed fusion (L-PBF) leads to the formation of coarse columnar β grains that give rise to anisotropic mechanical properties and inadequate strength. Incorporating the rare-earth oxide, yttrium oxide (Y2O3), has proven an effective strategy in enhancing the mechanical performance of Ti6Al4V alloys. Nevertheless, the critical Y2O3 content required to achieve an optimal strength–ductility balance in L-PBF Ti6Al4V has not been systematically determined. To address these critical gaps, this study, for the first time, systematically investigates the effect of various Y2O3 contents on the microstructural evolution and mechanical properties of Ti6Al4V alloys fabricated via L-PBF. The results demonstrate that a Y2O3 addition of 0.2 wt.% produces β grains and α phases with average sizes of 61.6 and 7.6 μm, respectively. Transmission electron microscopy observations reveal that Y2O3 nanoparticles, together with elemental Y nanoparticles formed by reduction, are distributed both within the α-Ti matrix and along phase boundaries. This distribution effectively reinforces grain boundaries and promotes heterogeneous nucleation, thereby refining the microstructure. Mechanical property tests indicate that the alloy strength significantly improves as the Y2O3 content increases. Specifically, the alloy with 0.2 wt.%Y2O3 exhibits a tensile strength of 1106 MPa, a yield strength of 1074 MPa, and an elongation of 10.7%. This study proposes an innovative rare-earth strengthening method for refining the microstructure of L-PBF-fabricated titanium alloys and comprehensively enhancing their mechanical properties.

1 May 2025 in Journal of Central South University
Verified
Journal Article
Closed access
PDF file
RLRen-Yi Lu
Ren-Yi Lu
GMGuonan Ma
Guonan Ma
GBGuan-Shun Bai
Guan-Shun Bai
WZWen-Tian Zhao
Wen-Tian Zhao
HZHui-Hua Zhang
Hui-Hua Zhang
XZXin-Peng Zhuang
Xin-Peng Zhuang

10 August 2026 in Coatings
Verified
Journal Article
Open access
PDF file
SZShuming Zhao
Shuming Zhao
YSYulin Sun
Yulin Sun
PYPengwei Yang
Pengwei Yang
YZYihan Zhou
Yihan Zhou
HZHuihua Zhang
Huihua Zhang
JHJianyu Hu
Jianyu Hu
Electron beam powder bed fusion (PBF-EB) of TiAl alloys exhibits different grain morphologies: equiaxed grains and columnar grains. However, the rule for controlling grain morphologies has not been found. In addition, the grain morphology is closely related to thermal gradient and growth velocity during PBF-EB. Here, thermal gradient and growth velocity are controlled by preheating temperature, beam current, and scanning speed. Based on the numerical simulation, the relationship between solidification parameters (thermal gradient and growth velocity) and process parameters (preheating temperature, beam current, and scanning speed) has been revealed. Meanwhile, the grain morphology of the topmost region of the PBF-EB-built Ti-48Al-2Cr-2Nb alloy can be controlled. In addition, the columnar-to-equiaxed transition is found in the PBF-EB-built Ti-48Al-2Cr-2Nb alloy. This is attributed to the PBF-EB technology belonging to the layer-by-layer stacking process, and the stacked layer reduces the thermal gradient and increases growth velocity in the remelting region. These findings will contribute to understanding the grain morphology evolution of TiAl alloys during PBF-EB, providing the principle for controlling the grain morphology of PBF-EB-built TiAl alloys.

30 January 2026 in Preprints.org
Verified
Preprint
Open access
PDF file
JZJinyu Zhu
Jinyu Zhu
YDYangping Dong
Yangping Dong
HZHuihua Zhang
Huihua Zhang
SZShuming Zhao
Shuming Zhao
GMGuonan Ma
Guonan Ma
PXPeng Xu
Peng Xu
A Ti6Al4V alloy fabrication via laser powder bed fusion (L-PBF) leads to the formation of coarse columnar β grains that give rise to anisotropic mechanical properties and inadequate strength. Incorporating the rare earth oxide, yttrium oxide (Y₂O₃), has proven an effective strategy in enhancing the mechanical performance of Ti6Al4V al-loys. This study systematically investigates the effects of various Y₂O₃ contents on the microstructure and mechanical properties of Ti6Al4V alloys fabricated via L-PBF. The results demonstrate that a Y₂O₃ addition of 0.2 wt.% produces β grains and α phases with average sizes of 61.6 and 7.6 μm, respectively. Transmission electron microscopy observations reveal that Y₂O₃ nanoparticles, together with elemental Y nanoparticles formed by reduction, are distributed both within the α-Ti matrix and along phase boundaries. This distribution effectively reinforces grain boundaries and promotes heterogeneous nucleation, thereby refining the microstructure. Mechanical property tests indicate that the alloy strength significantly improves as the Y₂O₃ content in-creases. Specifically, the alloy with 0.2 wt.%Y₂O₃ exhibits a tensile strength of 1106 MPa, a yield strength of 1074 MPa, and an elongation of 10.0%. This study proposes an in-novative rare earth strengthening method for refining the microstructure of L-PBF-fabricated titanium alloys and comprehensively enhancing their mechanical properties.