Several affordable and pollution-free technologies have drawn a lot of attention because of the pressure of our energy needs and environmental problems; among these, thermoelectric technology has made enormous advances. It has been known that thermoelectric materials are efficient in transforming waste heat energy into electricity. The efficiency of thermoelectric materials is typically assessed using the ZT value, ZT = S2T/ρκ. Several methods have been highlighted in the literature for improving thermoelectric figure of merit. This review stands out for its particular emphasis on cutting-edge techniques that are leading to a new era of thermoelectric innovation, including doping, co-doping, alloying, nanostructuring, and nanocompositing. Our focus is on mid-temperature range thermoelectric materials, which operate between 500 and 900 K and have enormous potential for high-efficiency thermoelectricity and waste heat recovery due to their inherent thermal and electrical properties. This review provides a foundational understanding of thermoelectric concepts as well as obstacles to improving the figure of merit and the various classes of mid-temperature range thermoelectric materials, including their structure and thermoelectric characteristics are discussed in brief. Additionally, it also discusses different methods described in the various literature regarding enhancing performance as well as recent advancements made in this area and this article emphasizes the relevance and importance of these developments in the context of urgent global energy challenges and highlights the crucial role that mid-temperature range thermoelectric materials will play in determining the future landscape of sustainable energy sources. To satisfy the practical demand, scientific research in the field of thermoelectricity still needs to be intensified, for this mid-temperature range, Chalcogenide-based thermoelectric materials play a very important role in the future. Graphical
Thermoelectric materials possess the capability to convert electricity into heat and vice versa. The utilization of chlorofluorocarbons and hydrochlorofluorocarbons as thermal carrier agents in traditional cooling and air conditioning systems has sparked a surge in exploration toward pioneering refrigeration and spatial conditioning technologies. Chalcogenides, known for their capacity to amplify the thermoelectric efficiency of materials and their adaptability across a broad spectrum of temperatures, stand out as pivotal components in thermoelectric materials. Despite their existing suboptimal performance, these materials hold substantial promise as power generators and as solid-state Peltier coolers, attracting significant attention and positioning them as subjects ripe for further investigation. Categorized into alkali or alkaline earth, transition metal, and main-group chalcogenides, these materials and their respective subclasses are meticulously scrutinized to pinpoint the most suitable thermoelectric materials for specific applications with an optimal operational temperature span. In the quest for energy-efficient technologies characterized by simple designs, absence of moving components, and superior stability, thermoelectric materials play a crucial role. This review highlights the advancements in theoretical parameters as well as the figure of merit (ZT) of chalcogenide materials, emphasizing their device applications. These insights are intended to provide viable future approaches to mainstream thermoelectric materials. This review reveals that Cu2Se achieves a maximum ZT value of 2.66 at 1039 K, marking it as the top performer among transition metal chalcogenides. Conversely, SnSe, a main-group metal monochalcogenide, exhibits a ZT value of 2.8 at 773 K, whereas nanowires of the main group of bismuth chalcogenides exhibit a ZT value of 2.5 at 350 K.
One of the global demands of primary research objectives is to achieve human energy harvesting and self-powered wearable technologies. Bismuth chalcogenides are the trending materials for thermoelectric generators and Peltier coolers due to their notable thermoelectric figure of merit in the low- and room-temperature range. Systematic alloying of bismuth chalcogenides leads to a substantial change in their electrical and thermal transport properties. The high thermoelectric figure of merit (ZT) observed in bismuth chalcogenides is due to the rhombohedral crystal structure, lower effective mass, low thermal conductivity, and large band degeneracy. This review is aimed at identifying and quantifying different techniques for effectively improving the thermoelectric properties of doped/composite bismuth chalcogenide compounds. The review also examines the various synthesis methods including ball milling (BM), spark plasma sintering (SPS), self-propagating high-temperature synthesis (SHS), soft chemical reaction, hydrothermal reaction, melt growth (MG), melt spinning (MS), sintering and consolidated synthesis, and hot extrusion, with their respective figures of merit. Since device modification is a challenging task, this report reviews the present research on bismuth chalcogenide alloys to benchmark future development using various techniques. Graphical Abstract
21 September 2016 in Molecular Crystals and Liquid Crystals
Good-quality single crystals of an efficient nonlinear optical (NLO) chalcone derivative 1-(5-chlorothiophen-2-yl)-3-(2,3-dichlorophenyl)prop-2-en-1-one (CTDCP) which meets many of the physicochemical requirements like transparency in the entire visible region, thermal stability, mechanical hardness have been achieved. The crystal belongs to orthorhombic system with the centrosymmetric space group Pbca. The third-order NLO properties were investigated using a single beam Z-scan technique with nanosecond laser pulses at 532 nm. The nonlinear refractive index is found to be of the order of 10−11 cm2/W. The magnitude of third-order susceptibility is of the order of 10−13 esu. The compound exhibits good optical limiting at 532 nm. The mechanical property of the crystals showed load dependent hardness. The static and frequency dependent molecular hyperpolarizabilities were computed using MOPAC 2012. Thermal study confirms that the crystal is dimensionally stable up to 179°C. The influence of direction of charge transfer on the nonlinearity of the molecule has been discussed in detail.