Controlling prior austenite morphology during single-pass hot rolling is essential for improving the strength–ductility balance of strip casting high-strength steels. In this study, Fe–0.24C–1.5Si–1.8Mn steels with and without 0.03 wt.% Nb were deformed by 50% at 950–1100 °C and subsequently held at 350 °C for 60 min for bainitic transformation. The effects of deformation temperature and Nb addition on austenite dynamic recrystallization, bainitic microstructure, and mechanical properties were investigated. For the Nb-free steel, recrystallization occurred at all these investigated deformation temperatures. The addition of 0.03 wt.% Nb markedly suppressed austenite recrystallization during hot deformation, resulting in the retention of elongated deformed austenite after deformation at 950 °C. Compared with the bainitic microstructure formed from fine recrystallized austenite in the 0Nb steel (without Nb addition), that formed from elongated austenite in the 03Nb steel (with 0.03 wt.% Nb) deformed at 950 °C exhibited a smaller lath width and higher HAGB and dislocation densities. In addition, the volume fraction of retained austenite increased from 4.5% to 9.8%, while its average thickness decreased from 105.6 nm to 49.1 nm. Consequently, under identical deformation conditions (50% reduction at 950 °C), Nb addition increased the yield and tensile strengths from 1064 MPa and 1261 MPa to 1088 MPa and 1323 MPa, respectively, while the total elongation remained nearly unchanged (24.8% vs 24.6%). These findings provide new insights into the optimization of thermomechanical processing for strip casting bainitic steels.
The increasing use of electric arc furnace (EAF) in steelmaking inevitably elevates nitrogen (N) levels, which are traditionally regarded as a detrimental element to the formability of ultra-low carbon (ULC) steels due to the formation of Lüders band. Here, we demonstrate that N could act as a beneficial microalloying element in strip casting ULC steels by promoting V(C, N) precipitation and grain refinement of ferrite. Thermodynamic calculations reveal that N significantly increases both the equilibrium volume fraction and equilibrium precipitation temperature of V(C, N), enabling copious interphase nanoprecipitation during ferrite transformation. Microstructural characterization confirms the enhanced formation of V(C, N) within interphase rows in the N-containing steels, leading to greater Zener pinning effect and smaller ferrite grain size (from 7.50 μm of 0N to 4.67 μm of 96 ppm N and 3.84 μm of 139 ppm N). As a result, owing to the enhanced nanoprecipitation and grain refinement, the N-containing ULC strip casting steels exhibit a superior strength–ductility synergy, with tensile strength increased from 666 MPa (0N) to 805 MPa (96 ppm N) and 825 MPa (139 ppm N), and a slight decrease in total elongation from 29.8% (0N) to 27.3% (96 ppm N) and 22.0% (139 ppm N). In addition, no Lüders plateau was observed in the tensile stress-strain curves as the extensive formation of V(C, N) consumed the N atoms in solid solution. These findings highlight that microalloying V in the steels produced by EAF can effectively leverage the high N content for achieving superior strength–ductility synergy.