Poly (ether ether ketone) (PEEK) has attracted increasing attention for dental applications because of its favorable mechanical properties, physicochemical stability, and biocompatibility. However, its inherently poor bonding characteristics remain a major limitation in clinical practice. This study investigated the effect of sequential alumina airborne-particle abrasion (sandblasting) followed by plasma treatment on the bonding performance of methyl methacrylate (MMA)-based luting systems to dental CAD-CAM PEEK. PEEK specimens were prepared as plates and divided into four surface-treatment groups: untreated, airborne-particle abraded, plasma-treated, and airborne-particle abraded followed by plasma treatment. Surface characteristics were evaluated using SEM–EDX analysis and surface roughness measurements, and surface wettability was assessed by contact angle measurements using primers from two MMA-based luting systems (Beautylink [BL] and Super-Bond [SB]). Shear bond strength (SBS) between treated PEEK and each luting system was determined after 24 h of water storage (initial) and after 20,000 thermocycles (aged). Airborne-particle abrasion significantly increased surface roughness, whereas plasma treatment enhanced surface wettability without altering roughness. The combined treatment resulted in the highest surface roughness and the lowest contact angles and demonstrated superior or comparable SBS compared with the single treatments. After aging, the combined treatment significantly improved bonding durability. These findings indicate that airborne-particle abrasion followed by plasma treatment enhances the bonding performance and durability of MMA-based luting systems to PEEK.
1 January 2024 in Annals of Japan Prosthodontic Society
This study investigated the effect of CAD-CAM resin composite thickness on the polymerization behavior of dual-cure resin cements used for endocrown restorations. Three commercially available dual-cure resin cements and one light-cure resin cement (for comparison) were polymerized by light irradiation through CAD-CAM resin composite plates of varying thicknesses (1.5, 3.5, 5.5, 7.5, and 9.5 mm). Transmitted light intensity was measured using an optical spectrometer. Polymerization behavior was evaluated immediately after irradiation and after 24 h of aging using Fourier transform infrared spectroscopy to determine the degree of conversion (DC) and Vickers hardness (VH) testing. Transmitted light intensity decreased logarithmically with increasing composite thickness, with less than 1% of incident light reaching the resin cement at thicknesses ≥ 5.5 mm. For the dual-cure resin cements, DC and VH values significantly decreased when the composite thickness exceeded 5.5 mm. Although DC and VH increased after 24 h due to self-curing, values beneath thicker composites remained lower than those beneath 1.5 mm thick composites. The light-cure resin cement failed to polymerize when the composite thickness exceeded 7.5 mm. These results indicate that CAD-CAM resin composite thickness critically influences resin cement polymerization, highlighting the importance of thickness control in endocrown restorations.
1 January 2026 in Asian Pacific Journal of Dentistry
This case report describes a patient with obstructive sleep apnea (OSA) who could not receive oral appliance therapy because of temporomandibular disorders and was instructed to perform tongue rotation exercises. The patient’s maximum tongue pressure, lip-seal strength, and subjective sleep quality improved post-intervention. Furthermore, apnea-hypopnea index and sleep architecture were improved after exercise compared with the baseline. These results suggest that tongue rotation exercises can improve not only oral function but also respiratory function during sleep and, thus, may be meaningful to introduce as an adjunctive therapy for OSA with impaired oral function or intolerance to conventional therapies.
This study evaluated the effects of the methyl methacrylate (MMA)-containing adhesive primer Visio.link on the surface characteristics of sandblasted poly(ether ether ketone) (PEEK) and its bond strength to four dental resin cements: the MMA-based resin cement Super-Bond EX (SB) and the composite-based resin cements RelyX Universal Resin Cement (RX), G-CEM LinkForce (GC), and Panavia V5 (PA). Sandblasted PEEK specimens were tested with or without primer application. Surface morphology, surface roughness, and surface free energy were evaluated, and shear bond strength (SBS) was measured after 1 day of water storage and after 20,000 thermal cycles. Primer application smoothed the sandblasted surface, reduced surface roughness, increased the polar component, and decreased the dispersive component and total surface free energy. Primer application significantly increased the initial SBS of RX, GC, and PA; however, thermal aging reduced bonding durability and caused pretest debonding in several groups. For SB, primer application did not significantly affect the initial SBS, whereas the sandblasted group showed significantly higher SBS than the primer-treated group after aging. The effect of the MMA-containing primer therefore depended on resin cement type and aging condition. These findings suggest that primer application should be considered according to the composition and bonding mechanism of the resin cement rather than routinely incorporated into PEEK bonding procedures.