Bismuth ferrite (BiFeO3) is a promising material for developing the next generation of multifunctional electronic devices. However, the production of high-quality BiFeO3 thin films is compromised by the tendency for structural and electronic defects to form during synthesis, which degrades their functional properties. In this work, BiFeO3 thin films were prepared by chemical solution deposition to determine optimal conditions for minimizing oxygen vacancies and to evaluate the impact of these point defects on their physical properties. The films were pyrolyzed at 300 °C for 60 min and 360 °C for 10 min, and crystallized in air and in an O2 atmosphere, at 600 °C and 640 °C for 40 min. High oxygen vacancies were observed in films prepared at low pyrolysis temperatures and crystallized in air, whereas oxygen vacancies were minimized in the film pyrolyzed and crystallized at high temperatures in an O2 atmosphere. The oxygen vacancies markedly affected the films’ physical properties, leading to increased dielectric loss, dielectric dispersion, dc conductivity, and leakage current, with consequent degradation of photovoltaic and magnetic performance. These findings highlight the critical importance of controlling synthesis parameters to suppress oxygen vacancy formation and achieve high-quality BiFeO3 thin films.
We report studies on the unusual frequency dispersion of the dielectric permittivity maxima of methylammonium lead iodide pellets at temperatures around the tetragonal–cubic phase transition. The origin of this observed permittivity response was studied in terms of grains and grain boundaries’ contributions in impedance, electric modulus, dielectric permittivity, and electrical conductivity. From theoretical fits of impedance and electric modulus measurements at different temperatures over a frequency range of 103–10 Hz, the reconstructed contributions of the grain boundary and grain permittivities show peaks around 339 K and 384 K, respectively. The origin of the grain boundary permittivity peak is discussed in terms of heterogenic ionic conduction associated with I− and MA+ ions in MAPbI3, while the peak in grain permittivity at high temperature is in terms of ionization of intrinsic carriers. The high value of the grain dielectric permittivity , compared to the reconstructed grain boundary permittivity , suggests a possible relaxor ferroelectric behavior with a diffuse phase transition for methylammonium lead iodide. The difficulties in confirming the ferroelectric nature of this halide perovskite based on impedance and electrical module data are also discussed.
The impact of defects on the electrical properties of bismuth ferrite thin films has been studied. Secondary phases and oxygen vacancies were the main defects considered. Thin films with secondary phases show higher conductivities than single-phase films. Monophasic films annealed in oxygen atmosphere shows lower conductivity than the non-annealed film. For selected thin film with secondary phase, the relaxation in the grain boundary was predominant with activation energy eV, suggesting the first ionization oxygen vacancies as the relaxation mechanism in the studied films. The electric field effect on relaxation processes was similarly to Arrhenius thermally activated process.
Complex impedance and electric modulus spectroscopies were used to investigate the dielectric relaxation and conductivity of random oriented BiFeO3 thin films. Thermally activated charge transport models yielded activation energies of eV, which is consistent with an electrical conduction dominated by oxygen vacancies. The non-Debye behavior of impedance and electric modulus relaxations were modeled by Cole-Cole functions. Results suggest a coexistence of components from both long-range and localized relaxation in the studied BiFeO3 films dominated by grain boundaries. The dielectric relaxation induced by electric field does not follow the Arrhenius formalism.