Albert Joseph Feilzer

Prof. Dr. Albert Joseph Feilzer

orcid

Research Focus & Metrics

Academic Career Length

27Years (2000-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 October 2003 in Journal of Dental Research
Verified
Journal Article
Closed access
PDF file
AFAlbert Joseph Feilzer
Albert Joseph Feilzer
BDB.S. Dauvillier
B.S. Dauvillier
In this study, we explored the reduction of shrinkage stresses in restored teeth by stimulating viscous flow of adhesive restoratives during curing, by increasing the TEGDMA/BisGMA ratio in the resin of composite restoratives. We studied a series of experimental two-paste composites with different amounts of TEGDMA (30, 50, 70 wt%, respectively) in the resin by mechanical testing, infrared spectroscopy, and dilatometry, to determine how comonomer composition affects the mechanical and chemical properties of the composite during curing. It was found that the polymerization rate of BisGMA-TEGDMA composites is indicative of the viscoelastic behavior during curing: The higher the reactivity, the higher the stiffness and viscosity development. Composites with 50 wt% TEGDMA in the resin displayed the highest maximum polymerization rate. High amounts of TEGDMA in the resin only modestly increased the pre-gel viscous flow (= lowered viscosity) property of composites. Of these composites, high post-gel shrinkage is the decisive factor in high shrinkage stress development.

1 March 2018 in Journal of Dentistry
Verified
Journal Article
Closed access
MAMarwa Abdelaziz
Marwa Abdelaziz
IKIvo Krejci
Ivo Krejci
TPThomas Perneger
Thomas Perneger
AFAlbert Joseph Feilzer
Albert Joseph Feilzer
LVLydia Vazquez
Lydia Vazquez

1 November 2000 in Journal of Esthetic and Restorative Dentistry
Verified
Journal Article
Closed access
PDF file
BDBibi S. Dauvillier
Bibi S. Dauvillier
MAMaxim P. Aarnts
Maxim P. Aarnts
AFAlbert Joseph Feilzer
Albert Joseph Feilzer

13 May 2023 in Clinical Oral Investigations
Verified
Journal Article
Open access
PDF file
YLY Lu
Y Lu
Amanda Dal PivaAmanda Dal Piva
Amanda Dal Piva
INI Nedeljkovic
I Nedeljkovic
João Paulo Mendes TribstJoão Paulo Mendes Tribst
João Paulo Mendes Tribst
AFAlbert Joseph Feilzer
Albert Joseph Feilzer
CKCornelis J Kleverlaan
Cornelis J Kleverlaan
Objective: The objective of this study was to investigate the effects of glazing technique and firing on the surface roughness and flexural strength of an advanced lithium disilicate (ALD) and lithium disilicate (LD). Methods: Eight groups of bar-shaped specimens (1 mm × 1 mm × 12 mm, N=160, 20/group) were manufactured from ALD (CEREC Tessera, Dentsply Sirona) and LD (IPS e.max CAD, Ivoclar). The specimens were then submitted to various posttreatments: crystallization (c), crystallization followed by a second firing (c-r), crystallization with glaze in one step (cg), and crystallization followed by a glaze layer firing (c-g). Surface roughness was measured by means of a profilometer, and flexural strength was determined using a three-point bending test. Surface morphology, fractography, and crack healing analysis were conducted using scanning electron microscopy. Results: Refiring (c-r) did not affect the surface roughness (Ra) while applying glaze at both cg and c-g procedures increased the roughness. ALDc-g (442.3 ± 92.5 MPa) promoted higher strength than ALDcg (282.1 ± 64.4 MPa), whereas LDcg (402.9 ± 78.4 MPa) was stronger than LDc-g (255.5 ± 68.7 MPa). Refiring completely closed the crack in ALD, but it had a limited effect on LD. Conclusions: Two-step crystallization and glazing improved ALD strength compared to the one-step protocol. Refiring and one-step glazing do not increase LD’s strength, while two-step glazing has a negative effect. Clinical relevance: Besides both materials being lithium-disilicate glass ceramics, the glazing technique and firing protocol affected their roughness and flexural strength differently. A two-step crystallization and glazing should be the first choice for ALD, while for LD, glazing is optional and when necessary, should be applied in one-step.

28 July 2008 in Contact Dermatitis
Verified
Journal Article
Closed access
PDF file
AFAlbert Joseph Feilzer
Albert Joseph Feilzer
RLR. Laeijendecker
R. Laeijendecker
CKC. J. Kleverlaan
C. J. Kleverlaan
PSP. Van Schendel
P. Van Schendel
JMJ. Muris
J. Muris

8 September 2022 in Contact Dermatitis
Verified
Journal Article
Open access
NGNiels P. J. De Graaf
Niels P. J. De Graaf
SRSanne Roffel
Sanne Roffel
SGSue Gibbs
Sue Gibbs
CKCornelis J Kleverlaan
Cornelis J Kleverlaan
MGMarta Lopez Gonzalez
Marta Lopez Gonzalez
HBHetty J Bontkes
Hetty J Bontkes
Background: Nickel‐induced proliferation or cytokine release by peripheral blood mononuclear cells may be used for in vitro diagnosis of nickel allergy.Objectives: Aim of this study was to explore the nickel‐specific cytokine profile to further elucidate the pathogenesis of nickel allergic contact dermatitis (ACD) and to identify potential new biomarkers for nickel ACD.Methods: Peripheral blood mononuclear cells from patients and controls were cultured with T‐cell skewing cytokine cocktails and/or nickel. Cytokine and chemokine concentrations were assessed in culture supernatants using validated multiplex assays. Specific cytokine production was related to history of nickel allergy and patch‐test results.Results: Twenty‐one of the 33 analytes included in the analysis were associated with nickel allergy and included type1 (TNF‐α, IFN‐γ, TNF‐β), type 2 (IL‐3, IL‐4, IL‐5, IL‐13), type 1/2 (IL‐2, IL‐10), type 9 (IL‐9), type 17/1 (IL‐17A[F], GM‐CSF, IL‐21) and type 22 (IL‐22) derived cytokines as well as the T‐cell/antigen presentation cell derived factors Thymus and activation regulated chemokine (TARC), IL‐27 and IP‐10. Receiver operator characteristics (ROC) analysis showed that IL‐5 was the strongest biomarker for nickel allergy.Conclusions: A broad spectrum of 33 cytokines and chemokines is involved in the allergen‐specific immune response in nickel allergic patients. IL‐5 remains, next to the lymphocyte proliferation test, the strongest biomarker for nickel allergy.