The growth behavior of laser-induced damage sites is affected by a large number of laser parameters as well as site morphology. Here we investigate the effects of pulse duration on the growth rate of damage sites located on the exit surface of fused silica optics. Results demonstrate a significant dependence of the growth parameters on laser pulse duration at 351 nm from 1 ns to 15 ns, including the observation of a dominant exponential versus linear, multiple-shot growth behavior for long and short pulses, respectively. These salient behaviors are tied to the damage morphology and suggest a shift in the fundamental growth mechanisms for pulses in the 1-5 ns range.
Growth of laser damage on fused silica optical components depends on several key parameters including laser fluence, wavelength, pulse duration, and site size. Here we investigate the growth behavior of small damage sites on the exit surface of SiO2 optics under exposure to tightly controlled laser pulses. Results demonstrate that the onset of damage growth is not governed by a threshold, but is probabilistic in nature and depends both on the current size of a damage site and the laser fluence to which it is exposed. We also develop models for use in growth prediction. In addition, we show that laser exposure history also influences the behavior of individual sites.
We present a comprehensive statistical model which includes both the probability of growth and growth rate to describe the evolution of exit surface damage sites on fused silica optics over multiple laser shots spanning a wide range of fluences. We focus primarily on the parameterization of growth rate distributions versus site size and laser fluence using Weibull statistics and show how this model is consistent with established fracture mechanics concepts describing brittle materials. Key growth behaviors and prediction errors associated with the present model are also discussed.
The structure of single crystals (so-called KDP) irradiated with , 355 nm laser pulses with fluences above the laser-induced breakdown threshold is studied by a combination of Raman scattering, photoluminescence, and soft x-ray absorption spectroscopies. We compare spectra from the as-grown material, surface and bulk laser-induced damage sites, as well as from references. Results show that irradiation with fluences above the laser-induced breakdown threshold leads to decomposition of KDP at surface damage sites but not at bulk damage sites. New spectroscopic features are attributed to dehydration products. For the laser irradiation conditions used in this study, the decomposed near-surface layer absorbs photons at (364 nm). These results may explain the recently reported fact that surface laser damage sites in KDP crystals tend to grow with subsequent exposure to high-power laser pulses, while bulk damage sites do not.
The thin film damage competition series at the Boulder Damage Symposium provides an opportunity to observe general trends in laser damage behavior between different coating types (high reflector, antireflector, polarizer, and Fabry–Perot filter), wavelength ranges (193 to 1064 nm), and pulse length ranges (40 fs to 18 ns). Additionally, the impact of deposition process, coating material, cleaning process, and layer count can be studied within a single year or more broadly across the history of this competition. Although there are instances where participants attempted to isolate a single variable to better understand its impact on laser resistance, this series of competitions isolates the variable of the damage testing service and protocol for a wide variety of participants to enable the observation of general trends. In total, 275 samples from 58 different participants have been tested at four different laser damage testing facilities over the last 10 years. Hafnia was clearly the best high refractive index material except for ultraviolet (UV) applications, although a wide range of high refractive index materials performed well. The best deposition process varied significantly between the different competitions. The best deposition process was dependent on the coating type, wavelength, and pulse duration. For 1064-nm coatings with nanosecond scale pulse lengths, e-beam coatings tended to be the best performers. For short-pulse length NIR mirrors and nanosecond pulse length UV mirrors, densified coating processes, which all involved sputtering of the target material, were the best performers. For UV antireflector (AR) coatings and excimer mirrors, both tested at nanosecond pulse lengths, they tended to favor very low energetic deposition methods yielding soft coatings, such as sol gel dip coating for the AR and resistive heating of fluorides for the excimer mirrors. Finally, cleaning method and layer count had a less obvious correlation with laser resistance over the history of this thin film damage competition series.
The dynamics of material response following initial localized energy deposition by the laser pulse on the material's surface is still largely unknown. We describe a time-resolved microscope system that enables the study of the sequence of events and the individual processes involved during the entire timeline from the initial energy deposition to the final state of the material, typically associated with the formation of a crater on the surface. To best capture individual aspects of the damage timeline, this system can be configured to multiple imaging arrangements, such as multiview image acquisition at a single time point, multi-image acquisition at different time points of the same event, and tailored sensitivity to various aspects of the process. As a case example, we present results obtained with this system during laser-induced damage on the exit surface of fused silica.