Co additions to titanium aluminides were assessed to decrease the typically high sintering temperatures necessary for the densification of intermetallics. Compositions based on the binary Ti-45Al with ternary Co variations between 1-10 at.% were investigated. The specimens were cylinders with 8 mm diameter prepared using blended elemental powders followed by cold uniaxial pressing. Sintering was carried out under an argon atmosphere at different temperatures ranging from 1100 to 1400 °C for 2 hours in a tube furnace. The results indicated that there was a systematic increase in densification with Co additions. The relative density of the reference material Ti-45Al was approximately 53%, however, Co addition of 10% led to densifications in the order of 80%. A strong effect of decreasing the sintering temperature was achieved with Co additions. The microstructure changed from fully lamellar with 1 at.% Co sintered at 1400 °C to duplex with higher Co additions sintered at 1200 °C. Besides the γ-TiAl and α2-Ti3Al equilibrium phases, the formation of a CoAl2Ti intermetallic was identified. The addition of 7% Co led to the highest hardness of approximately 450 HV.
One of the most effective approaches for the densification of titanium aluminides processed by powder metallurgy involves the addition of elements that induce the formation of a liquid phase during sintering. This work investigated the sintering behavior and creep resistance of Ti-45Al (in at.%) with ternary Co or Ni additions. Conventional sintering under a high vacuum atmosphere led to densifications of approximately 90% of the theoretical density in the Ti-45Al-2Co and Ti-45Al-2Ni alloys, while binary Ti-45Al was limited to a maximum of 57%. Microstructural analysis revealed the formation of equilibrium intermetallics γ-TiAl and α2-Ti3Al, along with Ni- and Co-rich regions concentrated at the boundaries of primary particles. Compression creep tests at 800°C under a 120 MPa load demonstrated a significant increase in mechanical strength, especially with the addition of Co, which showed 1% of plastic deformation in approximately 18 hours.
Laser processing has been widely investigated as an effective approach for improving surface properties and consolidating advanced materials, particularly complex alloys such as titanium aluminides (TiAl). In this study, laser surface remelting was applied to binary (Ti-45Al) and ternary (Ti-45Al-2Co and Ti-45Al-2Ni) alloys produced by powder metallurgy via blended elemental (BE) and pre-alloyed (PA) powder routes. Laser powers of 50 and 100 W were employed, resulting in a high-energy-density surface remelting regime applied to both green compacts and sintered samples with relatively high initial porosity, under an argon-controlled atmosphere. Microstructural and phase analyses were performed using scanning electron microscopy (SEM) and X-ray diffraction (XRD), while mechanical behavior was assessed by instrumented microindentation. Laser processing promoted the formation of a dense and homogeneous surface layer, approximately 150 μm thick, accompanied by significant microstructural refinement and enhanced hardness and elastic modulus. While rapid solidification led to crack formation in laser-treated sintered samples, the green compacts exhibited defect-free modified layers. Overall, the results demonstrate that laser surface remelting is an effective strategy for enhancing the surface integrity and mechanical performance of TiAl alloys processed by powder metallurgy.
Super duplex stainless steels (SDSS) combine excellent mechanical strength and corrosion resistance but may undergo microstructural degradation when exposed to temperatures between 400 and 1010 °C, due to the precipitation of deleterious intermetallic phases such as the sigma (σ) phase. This study investigates the phase evolution in UNS S32750 SDSS subjected to aging treatments at 850, 900, and 950 °C for 10, 100, and 1000 min, followed by water quenching and furnace cooling. The surface and phase microhardness, as well as the volume fraction and average grain size of the σ-phase, were evaluated. The results showed an increase in microhardness with both temperature and aging time, reaching a maximum of 418 ± 4 HV₀.₅ under the 850 °C / 1000 min condition. The σ-phase volume fraction remained nearly constant after 1000 min, regardless of the cooling method, while grain growth exhibited a similar trend across the three evaluated temperatures. These findings enhance the understanding of σ-phase precipitation and dissolution mechanisms and provide valuable insights for defining optimal thermal parameters in welding and manufacturing processes involving UNS S32750 super duplex stainless steel.