Many promising applications of single crystal diamond and its color centers as sensor platform and in photonics require free-standing membranes with a thickness ranging from several micrometers to the few 100 nm range. In this work, we present an approach to conveniently fabricate such thin membranes with up to about one millimeter in size. We use commercially available diamond plates (thickness 50 m) in an inductively coupled reactive ion etching process which is based on argon, oxygen and SF . We thus avoid using toxic, corrosive feed gases and add an alternative to previously presented recipes involving chlorine-based etching steps. Our membranes are smooth (RMS roughness <1 nm) and show moderate thickness variation (central part: <1 m over ≈200 × 200 m ). Due to an improved etch mask geometry, our membranes stay reliably attached to the diamond plate in our chlorine-based as well as SF -based processes. Our results thus open the route towards higher reliability in diamond device fabrication and up-scaling.
We report on direct, real-space imaging of the stray magnetic field above a micro-scale disc of a thin film of the high-temperature superconductor YBa2Cu3O7−δ (YBCO) using scanning single spin magnetometry. Our experiments yield a direct measurement of the sample’s London penetration depth and allow for a quantitative reconstruction of the supercurrents flowing in the sample as a result of Meissner screening. These results show the potential of scanning single spin magnetometry for studies of the nanoscale magnetic properties of thin-film superconductors, which could be readily extended to elevated temperatures or magnetic fields.
Nanoscale magnetic stray fields of two materials are measured with an NV center scanning probe. Quantitative imaging of the Meissner effect of a superconductor allows for reliable determination of the London penetration depth. Stray fields of the 2D vdW magnet CrI3 provide evidence for antiferromagnetic coupling in the few-layer sample.