A calculation model of surface tension for molten slags in SiO2–Al2O3–CaO–MgO systems has been developed in the present study, based on a statistical modelling approach. A total of 832 experimental data of slags have been critically selected and used for the optimization of model parameters, and the present model has a fairly lower average deviation with 4.60% within the applicable composition and temperature ranges. And also, the composition and temperature dependences of surface tension have been discussed using the model. The results indicate that the surface tensions always decrease with increasing SiO2 content and increase with increasing MgO content. The surface tension will decrease with increasing temperature.
Nickel slag is a metallurgical solid waste from nickel refineries, which can be recycled as one of excellent secondary sources due to valuable iron contents. In this work, the approach of recycling nickel slag by aluminum dross was proposed, and the processes of network modification of slags and reduction were successively investigated at 1773 K. Upon the thermodynamic calculations, CaO was chosen as the modifier in order to obtain a higher activity of ‘FeO', and basicity of the modified slag was determined as 1.0. Element mapping analysis of the modified slag showed that ‘FeO' had been separated from the structure of nickel slag. After aluminothermic reduction for 120 min, the recovery degree of iron and copper was 94.35% and 97.89%, respectively. In addition, the secondary slag stabilization was discussed, and the utilization of the produced Fe–Cu alloy and the secondary slag was analyzed.
8 February 2021 in Metallurgical and Materials Transactions B
Dissolution rate of limestone in converter slag is a key to evaluate the feasibility of limestone slagging mode during steelmaking process. In this work, kinetics of limestone dissolution in converter slag at 1300–1400°C were studied and the influence of decomposition reaction were investigated. The results showed that the dissolution process of limestone in converter slag can be divided into three stages: stagnation stage, coupling stage and sole dissolution stage. Higher slag temperature and lower slag basicity were conducive to reduce the duration time of stagnation stage and obtain higher dissolution degree. The coupling stage of limestone dissolution was confirmed to be controlled by the chemical reaction, whereas diffusion through the boundary layer as well as combination of controlling steps was the rate limitation at the sole dissolution stage under different slag basicities. The kinetics parameters were determined. In addition, CO2 bubbles generated from decomposition reaction could provide a certain enhancement of limestone dissolution and inhabit the formation of 2CaO·SiO2 phase at the coupling stage of limestone dissolution in converter slag.