Zeolite P was synthesized by hydrothermal treatment of coal fly ash and applied to the individual removal of six heavy metals (Pb2+, Ni2+, Cu2+, Cr3+, Hg2+, Cd2+) from aqueous solutions. Characterization by SEM-EDS, FTIR, BET, XRD, zeta potential, and XPS revealed a BET surface area of 30 m2/g, Si/Al ratio of 1.63, and pHpzc of 3.2. Batch experiments at the natural solution pH of 3.9 in all cases (C0 = 10, 100, 200 mg/L; t = 1–60 min) yielded an apparent selectivity sequence at C0 = 200 mg/L of Hg2+ (10.47 mg/g) > Pb2+ (9.12) > Ni2+ (2.18) > Cr3+ (2.05) > Cu2+ (1.82) > Cd2+ (1.26), where Hg2+ and Pb2+ reached near-equilibrium while the remaining metals were still approaching it at t = 60 min. Weber–Morris and Boyd analyses confirmed three sequential diffusion stages with a concentration-dependent shift from film to intraparticle diffusion control through the narrow GIS channels (3.1 × 4.5 Å). Ion exchange was identified as the dominant mechanism based on convergent kinetic, diffusion, XPS, and selectivity–electronegativity evidence (r = +0.76). A leakage-free machine learning framework combining physicochemical descriptors with experimental variables was tested under three cross-validation strategies of increasing stringency. Gradient Boosting achieved R2 = 0.979 ± 0.043 (repeated K-Fold) and R2 = 0.880 on six completely held-out kinetic curves. An ablation study confirmed that physicochemical descriptors are essential (experimental-only models yielded negative R2). SHAP feature importance rankings were consistent with established ion exchange selectivity theory. This work demonstrates that group-level validation, physics-informed descriptors, and systematic ablation testing are able to identify both the capabilities and the boundaries of small-dataset ML when testing for metal kinetics prediction.
1 October 2021 in Journal of Physics: Conference Series
We report the effective thermal properties at room temperature and proximate analysis of three mixtures of coke and carbon fines formed by uniaxial pressing at 30 MPa. Using differential scanning calorimetry and thermogravimetry, the thermal behavior of the carbon samples was determined. The KD2 Pro® system was used to measure the effective thermal properties, while the proximate analysis was carried out applying the ASTM D 3172-89 standard. It was found for coke fines that in the range between 40.00 °C and 293.94 °C there is a loss in weight of 3.2%, which corresponds to the degradation of low molecular weight volatiles, another degradation was also observed between 90.07 °C and 336.21 °C, and the maximum devolatilization temperature was 579 °C, finally from 700 °C the melting process begins, which corresponds to the formation of coke. It was also observed that the thermal conductivity increases with increasing coke concentration in the sample, and that the mixture with the highest thermal diffusivity was the one formed with 80% coke fines and 20% carbon fines. According to the thermal properties of the samples can be to be used efficiently as fuel.
A full-factorial 33 experiment was used in this study to determine the optimal values of the tensile properties of three composite materials manufactured based on three polymeric resins: Derakane Momentum epoxy vinyl ester based on bisphenol-A (DM-411), polyester based on terephthalic acid (P115-A), and isophthalic polyester (P2000). Such materials were reinforced with magnetite powders at concentrations of 10, 20, and 30 wt %, and the particle sizes were classified with three sieves: #200 (46–75 μm), #325 (26–45 μm), and #500 (0–25 μm). The compounds were manufactured using the hand lay-up method at room temperature in accordance with ASTM D638-14 for M1-type specimens. A tensile test was conducted on a universal Microtest EM2/300/FR machine at a test speed of 5 ± 25 % mm/min using an Epsilon extensometer calibrated in accordance with the ASTM E83 standard at 20 ± 2 °C. The magnetite powders and compound morphology were studied by Scanning Electron Microscopy. The mechanical properties of the compounds and the optimal response found by Analysis of Variance (ANOVA) and Response Surface Methodology (RSM) are also reported. The best response to the mechanical stimuli occurs with the composite material prepared with the epoxy vinyl ester resin DM-411, a concentration of 29.4 % of magnetite (Fe3O4), a particle size of 58.5 microns, and a 200 sieve.
1 October 2021 in Journal of Physics: Conference Series
The present work implements the Nicolson-Ross-Weir (NRW) method to find the permittivity and permeability through an algorithm in Matlab® of a magneto - dielectric composed material made of polyester resin and magnetite powders randomly dispersed and oriented vertically and horizontally in the polymeric matrix. The measured data come from the simulation of the S parameters in ADS® between 150 kHz and 4GHz, on a microstrip type transmission line. The algorithm allowed to verify that the best response in high frequency of the magneto - dielectric composed where the vertically orientedparticles, present the highest relative permittivity obtaining Er= 5.5 for 30% wt concentration and Er= 4.5 concentration of 20% wt, with an absorption coefficient which increases in function of frequency and the concentration of magnetite in the functional filler.